Micro-Arc Oxidation of Inner and Outer Surfaces of 6061 Aluminium Hollow Profiles for Wear-Resistant Applications
Furkan Yasa, Faiz Muhaffel
Key points
From the paper's conclusion- These results demonstrate that extended processing time can provide effective simultaneous protection of the internal and external surfaces of hollow aluminium profiles.
Abstract
Micro-arc oxidation (MAO) coatings were formed on 6061 aluminium alloy square hollow profiles to determine suitable processing conditions for achieving comparable coating characteristics and wear resistance on both inner and outer surfaces. The study specifically addresses the challenge of protecting internal surfaces of hollow aluminium components, which is important for wear-resistant lightweight profiles and structural sections used in automotive and aerospace applications. An aluminate-based electrolyte was employed, and the effects of processing potential and duration on coating development were systematically investigated. Coating phase composition, surface morphology, roughness, porosity, and thickness were characterised by X-ray diffraction (XRD), scanning electron microscopy (SEM), and 2D contact profilometry, while tribological performance was evaluated by reciprocating wear testing. Results showed that γ-Al2O3 was the dominant phase at shorter durations and lower potentials, with progressive formation of α- Al2O3 at higher potentials (≥480 V) or longer processing durations (10 min). The inner surfaces consistently developed thinner, less crystalline, and rougher coatings than the outer surfaces, which is attributed to geometric shielding within the confined cavity and is consistent with reduced discharge activity and restricted electrolyte circulation. Coating thickness increased with both processing time and potential, reaching approximately 24-25 µm on the outer surface and nearly 20 µm on the inner surface at the highest potential. At 390 V, the inner coating exhibited a wear volume loss nearly 300 times greater than the corresponding outer coating, demonstrating that process parameters selected solely according to outer-surface performance may be unsuitable for hollow components. In contrast, processing at 450 V for 10 min substantially reduced the inner–outer property difference and resulted in comparable wear resistance on both surfaces, with wear volume losses below 0.15 × 10-3 mm3. These results demonstrate that extended processing time can provide effective simultaneous protection of the internal and external surfaces of hollow aluminium profiles.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- In situ preparation of wear- and corrosion-resistant micro-arc oxidized coatings enriched with the tetragonal-ZrO2 phase on 5052 aluminum alloy.Chemical communications (Cambridge, England) · 2026
- Microstructure and properties of a self-sealing MAO coating on 6063 aluminum alloy fabricated with stepwise current densityJournal of Materials Research and Technology · 2025
- The Investigation of the Electrode Soft-Mode Impact of Micro-Arc Oxidation (MAO) on the Structure, Phase Composition and Corrosion Properties of AlCa2.5Mn1.5 Aluminum Alloy Sheets with MAO Coating of Different ThicknessesJournal of Manufacturing and Materials Processing · 2026
- The Effect of Coarse-Grained and Ultrafine-Grained Ti13Nb13Zr Alloy Substrates on the Structure and Properties of Calcium Phosphate Coatings Formed by Micro-Arc OxidationCoatings · 2026
- Review of Preparation and Key Functional Properties of Micro-Arc Oxidation Coatings on Various Metal SubstratesCoatings · 2025
- In-situ synthesis of ZnO/CuO nanocrystals in micro-arc oxidation coatings for enhanced antibacterial performance and corrosion resistance of aluminum alloysJournal of Materials Research and Technology · 2025