Durability Performance of Geopolymer Mortar Incorporating Graphene Oxide and Additional Water Content

Nazirah Mohd Apandi, Alia Sofea Shamsol, Warid Wazien Ahmad Zailani, Nor Azian Aziz, Norhaida Mohamed

Key points

From the paper's conclusion
  • Overall, the study demonstrates that GO and water content must be carefully optimized to achieve balanced workability, controlled setting time, and improved potential durability in geopolymer mortar.

Abstract

This study investigates the combined influence of graphene oxide (GO) and additional water content on the fresh-state properties and early hardening behaviour of geopolymer mortar. Geopolymer mortar is increasingly recognised as a sustainable alternative to ordinary Portland cement-based materials; however, its performance is strongly governed by mixture workability, setting behaviour, pore structure, and matrix compactness. In this study, geopolymer mortar mixtures containing different GO dosages and water-to-powder (w/p) ratios were evaluated through flowability and setting time tests. Flowability was determined in accordance with ASTM C1437, while setting time was measured using the Vicat Needle apparatus following ASTM C191. The results were further analysed using the Relative Flowability Index (RFI) and Modified Flow Consistency Index (MFCI). The findings showed that increasing GO content reduced mortar flowability due to the high surface area, nanosheet morphology, and water absorption capacity of GO, which increased mixture cohesion and restricted particle movement. The RFI decreased from 100% for the control mixture to 79.74% at 0.10% GO, indicating significant loss of flowability. However, increasing the w/p ratio partially improved flow consistency by enhancing particle dispersion and mixture deformability. Setting time results showed that GO accelerated early stiffening, with the initial setting time decreasing from 48 minutes to 38 minutes as GO dosage increased from 0% to 0.10%. Additional water moderated this acceleration by improving fluidity and reducing ionic concentration. Overall, the study demonstrates that GO and water content must be carefully optimized to achieve balanced workability, controlled setting time, and improved potential durability in geopolymer mortar. The findings provide new insights into the synergistic interaction between GO dosage and additional water content, contributing to the optimization of sustainable geopolymer mortar mixtures for practical construction and repair applications.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers