Beneath the Surface: An Analysis of the Role of Marble Waste Aggregate in Enhancing the Strength and Corrosion Resistance of Reinforced Concrete
Amira A. Al-Shereiqi, Khalifa S. Al-Jabri, Kazi M. Abu Sohel, M. K. Al Alawi
Key points
From the paper's conclusion- The results show that FC-MAW reduced workability due to the apparent difference in water absorption between MAW and natural aggregate.
Abstract
In recent years, the rapid growth of the marble manufacturing industry in Oman has resulted in a significant increase in marble waste (MAW), creating a major challenge for its disposal. To promote sustainable construction practices, MAW has been explored as a potential substitute to natural aggregates in concrete. In this study, both fine and coarse marble waste (FC-MAW) were used to replace both fine and coarse natural aggregates at replacement levels ranging from 0% to 100% in 25% increments, and their effects on concrete strength and durability were investigated. Properties including workability, hardened density, compressive strength, porosity, corrosion resistance using an accelerated impressed voltage test (ACTIV), and Scanning Electron Microscope (SEM) were determined. The results show that FC-MAW reduced workability due to the apparent difference in water absorption between MAW and natural aggregate. Compressive strength improved with higher replacement percentages and longer curing ages. Compared with the control mix (40.9 MPa at 28 days), the 28 day compressive strength increased by 4.7%, 11.6%, 16.1%, and 19.6% for the 25%, 50%, 75%, and 100% FC-MAW mixes, respectively (and by 6.1% to 15.2% at 7 days). Corrosion resistance also improved slightly, consistent with the porosity results, especially with higher FC-MAW. Specifically, increasing FC-MAW from 0% to 100% reduced the steel mass loss from 28.8% to 20.9% and the crack width from 4.1 mm to 2.0 mm, while delaying first crack initiation from 8 to 11 days. Furthermore, the correlation between compressive strength and cracking width becomes more obvious as the FC-MAW replacement increases. In corrosion tests, the weight loss of the steel reinforcing bar reduced with increasing replacement level. The study concluded that using FC-MAW as an aggregate could make concrete more durable in corrosion-prone areas, as evidenced by SEM.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Development of Sustainable Concrete Using Marble Waste Powder and Silica FumeIOP Conference Series: Earth and Environmental Science · 2026
- Mechanical and durability assessment of marble dust–fiber concrete supported by ML predictionScientific Reports · 2026
- Sulfuric acid corrosion resistance of recycled aggregate concrete containing magnetized waterScientific Reports · 2026
- Physical and Mechanical Properties and Partial Cradle-to-Gate Global Warming Potential of Mortars Incorporating Ecuadorian Waste Marble Powder as a Partial Cement ReplacementBuildings · 2026
- Microstructural properties of ordinary concrete mixed with rubber and plastic waste under aggressive environmental conditions: A full‐factorial design studyStructural Concrete · 2026
- Study on the Meso-Statistical Damage Constitutive Model of Coral Aggregate Seawater Concrete Incorporating Natural Aggregate Replacement Ratio Effects.Materials (Basel, Switzerland) · 2026