Statistical Assessment of Embodied Carbon in Geopolymer Mortars

Chenmeng Zhang, Dan V. Bompa, Natividad Garcia-Troncoso

Key points

From the paper's conclusion
  • The findings demonstrate the potential of geopolymer mortars to deliver substantial embodied carbon reductions at equivalent strength.

Abstract

This paper presents a statistical assessment of the relationship between compressive strength and embodied carbon for a database of 100 geopolymer mortar mixes, with comparison to conventional cement mortars. The geopolymer dataset covers a wide range of formulations and curing conditions, with 28-day compressive strengths between approximately 5 and 80 MPa and cradle-to-gate embodied carbon values ranging from 29 to 501 kgCO 2 eq/m 3 . Linear regression and distribution-based analyses were used to quantify trends and variability in strength-carbon relationships. The results indicate a positive correlation between compressive strength and embodied carbon for geopolymer mortars, although with substantial scatter reflecting differences in precursor chemistry and activator composition. At a compressive strength of approximately 20 MPa, the mean embodied carbon of geopolymers was approximately 170 kgCO 2 eq/m 3 . This represents a reduction of around 60-65% compared with typical embodied carbon values for cement-based mortars, which is approximately 460 kgCO 2 eq/m 3 . The lowest carbon geopolymer mix showed carbon reductions of more than 90% relative to cement-based mortars. The findings demonstrate the potential of geopolymer mortars to deliver substantial embodied carbon reductions at equivalent strength.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers