Hemp-Powered Mortar: A Sustainable Path to Improve Carbon Footprints
Kautik Bhutka, Tejas Joshi, Dinkey Mistry
Key points
From the paper's conclusion- This study investigates partial replacement of binder in plastering mortar with hemp hurds ( Cannabis sativa L.) at 1–5% by weight, using two binder systems UltraTech ReadyPlast and 53-grade OPC at 1:3 cement-to-sand ratio under water curing and 48-hour CO 2 -accelerated curing regimes.
Abstract
Cement manufacturing contributes approximately 7–8% of global anthropogenic CO 2 emissions, necessitating bio-aggregate substitution as a near-term decarbonisation strategy. This study investigates partial replacement of binder in plastering mortar with hemp hurds ( Cannabis sativa L.) at 1–5% by weight, using two binder systems UltraTech ReadyPlast and 53-grade OPC at 1:3 cement-to-sand ratio under water curing and 48-hour CO 2 -accelerated curing regimes. Hemp hurds with bulk density of 142 kg/m 3 and 24-hour water absorption of 10% were pre-wetted to saturated surface-dry condition prior to batching to maintain a constant effective water-to-binder ratio. Twelve mix proportions were cast as 70.6 mm cubes and tested for 7- and 28-day compressive strength, hardened density, and cradle-to-gate CO 2 footprint. Under water curing, the OPC system achieved peak 28-day compressive strength of 28.21 MPa at 2% hemp (84% of the 33.50 MPa control), declining to 19.81 MPa (59%) at 3% due to interfacial transition zone defects and localised paste desiccation. The ReadyPlast system exhibited a steeper regression slope of −4.54 MPa per 1% hemp versus −2.00 MPa for OPC; both systems satisfied IS 2250 MM 5 minimum of 5 MPa up to 4% replacement. CO 2 -accelerated curing proved detrimental above 2% hemp, reducing 7-day strength of the M5-RP mix by 40.5%, attributed to lumen-driven desiccation of the hurd–paste interface. Hardened density decreased from 2,134 kg/m 3 to 2,063 kg/m 3 at 4% hemp, yielding approximately 130 kg self-weight saving per 100 m 2 plastered floor. Cradle-to-gate life-cycle analysis yielded a net CO 2 reduction of 3% at 2% OPC replacement. The 2% OPC optimum is identified as technically and environmentally optimal for non-structural plastering in the Indian construction context.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Reaktive, CO 2 ‐negative Bindemittelkomponenten durch autotherme Co‐Pyrolyse von Algen, Textilabfällen und Tonce/papers · 2026
- Review and Evaluation of Agricultural Biomass Ashes as Supplementary Cementitious Materials for Sustainable ConcreteProcesses · 2025
- Novel process for valorising excavated clay to produce light weight aggregates by addition of carbonaceous residue, cement and CO2 curing.Waste management (New York, N.Y.) · 2026
- Unlocking the potential of bio-based composites: Durability and sustainability of hemp, flax, and miscanthus with low-carbon bindersResults in Engineering · 2026
- Portland Cement Mortar Incorporating Coffee Husk Ash as a Supplementary Cementitious Material: Preliminary Insights on Mechanical and Environmental PerformanceConstruction Materials · 2026
- Direct aqueous mineral carbonation of cementitious fines derived from hardened ready-mix concrete waste: Process performance and carbon accounting.Journal of environmental management · 2026