Achieving Optimal Dosing of Local Kaolinite Clay for Superior Mortar Properties
Safiya A. Al-Shereiqi, Khalifa S. Al-Jabri, Kazi M. Abu Sohel, Abdulaziz S. Al Maqbali, Mohammed Seddik Meddah
Key points
From the paper's conclusion- Therefore, 15% ADM-1 is the optimal replacement level, resulting in a significant enhancement in the performance of the blended mortar as a construction material.
Abstract
The increasing demand for diverse construction materials is essential for achieving sustainability and enhancing the performance of the construction industry. In this study, we examine how local Omani kaolinite clay might serve as a supplementary cementitious material by tuning its calcination conditions, which generally require less heat than conventional clinker production and therefore reduce the associated carbon footprint. Valorizing Omani clay also reduces reliance on imported pozzolans and the transport emissions associated with them, moving the construction sector toward lower-carbon, locally sourced materials. Therefore, the main aim of this study is to determine the optimal dosage of calcined clay (590°C for 2 hours), labelled ADM-1, sourced from Adam City, Oman, and to evaluate its effects on the fresh and hardened behavior of mortar. To achieve this objective, mortar mixtures with varying percentages of ADM-1 (0%, 5%, 10%, 15%, and 20% by weight) were assessed as replacements for Portland limestone cement (PLC), maintaining a constant mix ratio of 1:1.5:0.30 for cement, sand, and water-to-cement ratio. Fresh properties were measured, including fresh density and flowability. Additionally, the study investigated the hardened properties of the above-mentioned mixtures, including compressive and flexural strengths, ultrasonic pulse velocity (UPV), thermal conductivity, and scanning electron microscopy (SEM). The findings indicate that the fresh and hardened densities decreased with increasing calcined kaolin clay content in the mixtures, due to the lower specific gravity of ADM-1 (2.77) compared to the PLC (3.15). The optimal strength performance was achieved with 15% ADM-1 (PLC-15ADM-1), with relative compressive and flexural strengths at 28 days of curing of 118.9% and 112.7%, respectively. Moreover, UPV improved with increasing ADM-1 replacement in mortar, which can be attributed to microstructural densification resulting from pozzolanic reactions. This also led to a slight increase in thermal conductivity, up to 15% ADM-1 was added to the mortar mix, which then dropped at 20% ADM-1 replacement due to the cement dilution effect. Scanning electron microscopy (SEM) revealed a progressively denser microstructure with increasing ADM-1 content, characterized by reduced portlandite and a more continuous gel C-S-H/C-A-S-H gel, which corroborates the improvements in strength and UPV. Therefore, 15% ADM-1 is the optimal replacement level, resulting in a significant enhancement in the performance of the blended mortar as a construction material.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Low‐Carbon Composite Cement Mortar Incorporating Local Raw Materials as SCMs: Performance and Life Cycle AnalysisJournal of the American Ceramic Society · 2026
- Properties of alkali-activated materials incorporating calcined kaolin clay waste and blast furnace slagIOP Conference Series: Earth and Environmental Science · 2026
- Sustainable Design of Lightweight Low-Clinker Mortars Incorporating Recycled Ceramic ConstituentsEngineering Research Express · 2026
- Comparative Assessment of Calcined and Mechanically Activated Muscovite Clay as Supplementary Cementitious Materialce/papers · 2026
- Green cementitious materials: Utilization of soybean hull ash as a supplementary cementitious materialNext Materials · 2026
- Optimization of Multi-Component Cement Mortar Using a Taguchi Orthogonal Array Design.Materials (Basel, Switzerland) · 2026