Improving the dimensional stability of young clonal teak wood through fabrication of 3-layer cross-laminated timber (CLT)
Greitta Kusuma Dewi, Ragil Widyorini, Kaharuddin, Widiyatno, Sigit Sunarta, Fanny Hidayati, Ali Awaludin, Aqmal Nur Jihad,
Key points
From the paper's conclusion- This study aims to evaluate the dimensional stability of solid wood (raw material) and CLT made from 20-year-old thinned clonal teak wood.
Abstract
The utilization of young clonal teak is limited by its poor dimensional stability. Fabrication into cross-laminated timber (CLT) improves the property, as the orthogonal binding arrangement of layers reduces the anisotropic behaviour of wood. The degree of enhancement depends on both the wood species and the bonding performance. This study aims to evaluate the dimensional stability of solid wood (raw material) and CLT made from 20-year-old thinned clonal teak wood. Three-layer CLT (150 cm x 50 cm x 5.1 cm) was made and bonded using polyurethane at 160 g/m 2 glue spread under 1 MPa specific pressure. Dimensional stability was analyzed based on volumetric shrinkage, thickness swelling, and volumetric swelling, as well as changes after cyclic testing specifically for CLT. Results revealed that processing clonal teak wood into three-layer CLT substantially increased dimensional stability, as evidenced by reductions of 65% in mean volumetric shrinkage, 86% in mean volumetric swelling, and 63% in mean thickness swelling. CLT panels exhibited remarkable resilience, preserving structural integrity and dimensional stability through three successive cycles of cyclic testing. Fabricating 3-layer CLT from young clonal teak wood presents a practicable solution to enhance its utilization as a raw material for construction and furniture applications.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Potential of wood composites (particle board, oriented strand board and plywood) derived from rubber tree for cross-laminated timber productionJournal of Wood Science · 2026
- Bulk Modification of Wood Using a Combination of Hydrophobic Silica Sol-Gel and Nanoclay to Enhance Dimensional Stability and Durability.Materials (Basel, Switzerland) · 2026
- Additive-Free One-Step Hot Pressing of Radiata Pine for Simultaneous Surface Densification, Resin Exudation Suppression, and Dimensional StabilizationACS Sustainable Chemistry & Engineering · 2026
- Multiscale Interfacial Engineering Enables Robust Reconstituted Wood.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026
- Long-Term Bending Behaviour of Adhesive CLT Panel-to-Panel ConnectionsBuildings · 2026
- Buckling of adhesive-free Wooden-Dowelled Cross-Laminated Timber panelsEngineering Structures · 2025