  • The findings demonstrate that appropriate use of waste glass, depending on its particle size and application form, can enhance mechanical performance while promoting sustainable material utilization in AAMs.

Abstract

Alkali activated materials (AAMs) are a novel category of sustainable environmentally friendly construction materials, produced by the reaction of alkali activators such as sodium hydroxide solution (NaOH) or sodium silicate solution (Na2SiO3) with aluminosilicate materials, like fly ash (FA) or ground granulated blast furnace slag (GGBFS). AAMs offer reduced environmental impact, enhance durability and improved mechanical performance, making them a promising alternative for sustainable construction. Waste glass, a typical solid waste, contains rich silica and other active oxides, to recycle and reuse it in an environmentally friendly and effective way, adding it to AAM has become one of the feasible solutions to promote the development of green construction materials. Consequently, utilizing waste glass in the formulation of AAMs has emerged as a viable strategy to promote circular economic practices within the construction industry. To better apply waste glass to AAMs, this study investigates the integration of recycled waste glass into AAMs, with a focus on the impact of varying particle sizes on the distribution, mechanical properties, and microstructure of the material. Four distinct particle size fractions of waste glass will be evaluated: two fine glass powders with smaller particle sizes (less than 150μm) are used as binders, and the other two glass cullet with larger particle sizes (greater than 0.5mm) are used as aggregates. The mechanical properties of the AAMs will be evaluated through compressive strength testing at curing times of 7 and 28 days. For microstructural analysis, scanning electron microscope (SEM) and Energy Dispersive X-ray Spectroscopy (EDS) will be used to observe the distribution and interaction of waste glass particles within the AAMs matrix. This study explores the use of waste glass as both precursors binder and fine aggregates in AAMs, which can influence strength development differently depending on particle size and replacement rate. A Replacement Strength Index (RSI) is proposed to evaluate strength efficiency. The findings demonstrate that appropriate use of waste glass, depending on its particle size and application form, can enhance mechanical performance while promoting sustainable material utilization in AAMs.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Influence of Waste Glass with Varying Particle Sizes on the Mechanical Properties and Microstructure of Alkali Activated Materials — Science Skim