Genipin-crosslinked aligned PCL/gelatin/chitosan nanofibre scaffolds functionalised with PEDOT:PSS: electrical characterisation and cytotoxicity assessment using L929 fibroblasts.
Darius Čiužas, Vilma Petrikaitė
Institute of Cardiology, Lithuanian University of Health Sciences, Sukilėlių 13, Kaunas, Kaunas, 44307, Lithuania.
Key points
From the paper's conclusion- Here, we report aligned PCL/GE/CS nanofibre scaffolds fabricated using an acetic acid/acetone-based electrospinning route that avoids chlorinated solvents, crosslinked with genipin and subsequently functionalised by PEDOT:PSS dip-coating.
The optimised PCL/GE/CS stock-solution mixing ratio of 80:10:10 (v/v/v), corresponding to final polymer concentrations of 16.0, 1.0 and 0.2% (w/v), produced
Abstract
Electrospun polycaprolactone/gelatin/chitosan (PCL/GE/CS) composite nanofibre scaffolds are attractive for tissue engineering. However, their intrinsic electrical insulation limits electroactive applications. Here, we report aligned PCL/GE/CS nanofibre scaffolds fabricated using an acetic acid/acetone-based electrospinning route that avoids chlorinated solvents, crosslinked with genipin and subsequently functionalised by PEDOT:PSS dip-coating. The optimised PCL/GE/CS stock-solution mixing ratio of 80:10:10 (v/v/v), corresponding to final polymer concentrations of 16.0, 1.0 and 0.2% (w/v), produced uniform, bead-free aligned fibres with an average diameter of 356 ± 86 nm. Genipin crosslinking improved aqueous stability, with the scaffolds retaining approximately 98.9 ± 0.2% of their initial dry mass after 14 days in PBS compared with 95.4 ± 0.4% for the corresponding non-crosslinked PCL/GE/CS scaffolds, and reduced the 24 h swelling ratio from 440.8 ± 7.7% to 395.4 ± 9.3%. Subsequent genipin crosslinking and PEDOT:PSS coating slightly increased fibre diameter while preserving the aligned architecture. Surface characterisation confirmed PEDOT:PSS deposition by FTIR and SEM-EDX sulphur mapping. Wettability improved markedly: the water contact angle decreased from 143.2 ± 1.2° for PCL to 104.2 ± 2.4° for PCL/GE/CS and to 41.6 ± 6.2° after genipin crosslinking, while PEDOT:PSS-coated mats showed rapid droplet absorption. The conductivity was anisotropic, reaching 2.22 ± 0.15 S/m parallel to fibre alignment and 1.12 ± 0.06 S/m perpendicular to the fibre axis. In vitro studies with L929 fibroblasts showed no extract-mediated cytotoxicity under the tested conditions. Direct cell culture demonstrated increasing MTT metabolic activity from day 1 to day 7, while representative Live/Dead and DAPI/phalloidin images indicated sustained cell survival, attachment and cytoskeletal organisation. These findings demonstrate measurable electrical functionality together with L929 fibroblast compatibility and support further investigation of the scaffold as a candidate platform for electroactive tissue-engineering studies.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Evaluation of the Biological Response to Coating 3D-Printed PLA Scaffolds with Coaxial Gelatin-Based Electrospun FibersBiomimetics · 2026
- Synthesis and characterization of electrospun PCL-PVA-PPy-rGO fibers as a novel scaffold for bone tissue engineeringScientific Reports · 2026
- Investigating the crosslinking of an aligned, all-natural chitosan-gelatine-cellulose based polymeric scaffold for tendon tissue engineeringBiomaterials Advances · 2026
- Electrospun nanofibers and 3D-printed PCL/Chitosan-based scaffolds for advanced medical applications: a reviewAdvanced Composites and Hybrid Materials · 2026
- Recent advances of electrospun poly(L-lactide-co-ε-caprolactone) (PLCL) fibers for biomedical applications.Advances in colloid and interface science · 2026
- Bilayered PEDOT:PSS–Collagen Scaffolds as Functional Architectures for Tissue EngineeringAdvanced Materials Interfaces · 2026