Experimental and Analytical Characterization of Fused-Filament-Fabricated Polycarbonate: Coupled Effects of Raster Orientation and Printing Speed
Gaurang Patel, Vijaykumar Chaudhary, Kawaljit Randhawa
Key points
From the paper's conclusion- This study quantified the effects of unidirectional raster orientation (0°, 30°, 45°, 60° and 90°) and printing speed (30 and 60 mm s −1 ) using a balanced 5 × 2 design with six ASTM D638 Type I specimens per condition.
Abstract
Fused-filament-fabricated polycarbonate combines useful stiffness and impact resistance with process-created anisotropy arising from road alignment and inter-road interfaces. This study quantified the effects of unidirectional raster orientation (0°, 30°, 45°, 60° and 90°) and printing speed (30 and 60 mm s −1 ) using a balanced 5 × 2 design with six ASTM D638 Type I specimens per condition. Ultimate tensile strength (UTS), Young’s modulus, 0.2% offset yield strength and elongation at break were evaluated using two-way analysis of variance, an orientation-aware regression and a Hill–Tsai-type strength relation. Mean UTS decreased from 58.2 MPa at 0°/30 mm s −1 to 36.0 MPa at 90°/60 mm s −1 . Within this defined material–machine–setting combination and 30–60 mm s −1 speed interval, raster angle accounted for 94.8% of the observed UTS variation and printing speed for 3.6%, while their interaction was negligible for UTS. The same directional loss occurred in modulus, yield strength and elongation. The regression achieved an in-sample R 2 of 0.982 and a leave-one-angle-out R 2 of 0.944 (RMSE 1.64 MPa). After the Hill–Tsai parameters were frozen from the original ten condition means, 24 separately manufactured specimens at previously untrained 15° and 75° orientations were tested at both speeds. Across the four independent validation means, bias was −0.04 MPa, MAE 1.58 MPa, RMSE 1.59 MPa and R 2 = 0.951. This supports point prediction at the two new angles under the unchanged processing conditions, but not generalization to different materials, layups or process windows. Qualitative optical examination of representative fractures at 0°, 45° and 90° at both speeds showed a transition from predominantly intra-road rupture with well-developed inter-road necking at 0°, through mixed road/interface failure at 45°, to interface-dominated debonding, contour–infill separation and multiple apparent void-assisted initiation sites at 90°. The interface features and loss of apparent necking were more pronounced in the representative 60 mm s −1 specimens.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Experimental Investigation into the Influence of Infill Density, Print Pattern, and Built-Up Direction on the Flexural Strength of FFF-Manufactured PLA ComponentsJournal of Manufacturing and Materials Processing · 2026
- Flexural Behavior of Dual-Material PLA/ABS Specimens Manufactured by Fused Filament Fabrication: Effects of Raster Orientation, Deposition Strategy, and Material CompositionSymmetry · 2026
- Mesostructure, Toolpaths and the Finite-Element Prediction Gap in the Flexural Response of Planar and Non-Planar Fused Filament Fabrication.Polymers · 2026
- Ultra High Speed Fused Filament Fabrication of Carbon Fiber‐Reinforced PLA : A Comparative Study of TPMS ‐D and Gyroid Infill PatternsPolymer Composites · 2026
- Process, structure, and property relationships for carbon black-filled polylactic acid composite fabricated by fused filament fabrication: a mechanical performance studyREVIEWS ON ADVANCED MATERIALS SCIENCE · 2026
- Influence of Printing Orientation on Tensile Strength and Surface Characterization of a Steel-Powder-Reinforced Thermoplastic Composite Manufactured by FDM TechnologyMaterials · 2025