Effect of Artificial Aging Duration on the microstructural and hardness Behaviour of LM25-SiC-TiO 2 Hybrid MMC
S Prathap Singh, A Abishek Robert, R Kaushal
Key points
From the paper's conclusion- In this study, the effect of the artificial aging duration on microstructural changes and hardness behaviour of an Aluminium (Al) alloy (LM25) containing hybrid ceramic particles of Silicon Carbide (SiC) and Titanium Dioxide (TiO 2 ) was investigated.
Abstract
In this study, the effect of the artificial aging duration on microstructural changes and hardness behaviour of an Aluminium (Al) alloy (LM25) containing hybrid ceramic particles of Silicon Carbide (SiC) and Titanium Dioxide (TiO 2 ) was investigated. The 7.5 wt.% SiC and 2.5 wt.% TiO 2 hybrid metal matrix composite was produced by the stir-casting method. The ceramic reinforcements were added to the molten LM25 alloy in order to improve the mechanical properties and structural stability of the LM25 matrix. The fabricated composite specimens were solution treated for 4 hours at 550°C and then quenched and artificially aged for 4, 6 and 8 hours at 250°C. The as-cast condition was kept to serve as the control condition. Optical microscopy, X-ray Diffraction (XRD), and Vickers microhardness were used to assess the effect of aging time. The microstructural analysis confirmed the presence of uniformly distributed SiC and TiO 2 particles in the Al matrix, and heat treatment induced changes in the eutectic Silicon (Si) morphology and precipitation behavior. The 6-hour aging condition yielded a rather fine and uniform microstructural structure, along with a more uniform distribution of reinforcement and precipitation strengthening. The occurrence of Al, SiC, TiO 2 and Si phases was authenticated by XRD with no notable amounts of undesirable reaction products. Maximum hardness was achieved at 6 hours of the artificial aging, which is about 37% more than the as-cast condition. The lower hardness measured at 4 hours was caused by insufficient precipitation, while long aging at 8 hours caused coarsening of the precipitates and loss in strengthening.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Enhanced Mechanical Performance of Al7075/ 3–9 wt % SiC and 2 wt % Al 2 O 3 Hybrid Composites Through T6 Heat TreatmentAdvances in Materials Science and Engineering · 2026
- Influence of Silicon Carbide and Red Mud Reinforcements on the Mechanical Behaviour of Al6061 Hybrid CompositesJournal of Physics: Conference Series · 2026
- Comparative Evaluation of Single and Hybrid Reinforcements in Aluminum Matrix Composites: Effects of SiC, Si3N4 and TiO2 Content on Mechanical and Tribological PropertiesSustainability · 2026
- Nanoparticle-reinforced Aluminium Matrix Hybrid Composites: Processing and CharacterizationJournal of Environmental Nanotechnology · 2026
- Effect of particulate reinforcement on the aging behavior of aluminium metal matrix composites - A reviewJournal of Materials Research and Technology · 2025
- Influence of cryogenic treatment on the microstructure and mechanical behaviour of Aluminium-Silicon Carbide-Graphite compositesDiscover Applied Sciences · 2026