Key points
From the paper's conclusion- The results indicate that coating thickness, permeability, and spatial distribution should be jointly optimized while avoiding excessive weakening of the pole-tooth substrate.
Abstract
To address corrosion of ferromagnetic pole pieces in ferrofluid seals for chemical pumps handling corrosive media, a two-dimensional axisymmetric Maxwell magnetostatic model of a laser-cladded ferrofluid seal was established with fixed pole-tooth geometry and a final sealing gap of 0.10 mm. The effects of coating thickening mode, equivalent relative permeability, and thickness nonuniformity on the magnetic field and theoretical sealing pressure were investigated. The results show that increasing the thickness of a low-permeability coating reduces the magnetic-field peak and peak-to-valley difference. For the external-build-up model, the sealing pressure decreases from 0.356 MPa to 0.156 MPa as the coating thickness increases from 0 to 0.40 mm. The embedded-build-up model further weakens the 2Cr13 magnetic-conduction cross-section, resulting in only 0.100 MPa at 0.30 mm, 46.5% lower than the external-build-up model. Increasing the coating permeability from 1 to 100 raises the sealing pressure from about 0.23 MPa to 0.49 MPa, but the improvement becomes limited beyond μ r =20. High-permeability coatings also induce a double-peak magnetic-field profile by shifting the effective magnetic-pole boundary. For nonuniform coatings, tooth-top/tooth-side redistribution increases the pressure from 0.321 MPa to 0.340 MPa, while a three-zone asymmetric scheme reaches 0.421 MPa. The results indicate that coating thickness, permeability, and spatial distribution should be jointly optimized while avoiding excessive weakening of the pole-tooth substrate.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Structural Optimization Simulation of Non-Uniform Pole Teeth in Ferrofluid Seals Based on Multi-Stage Pressure-Bearing BalanceJournal of Physics: Conference Series · 2026
- Study on viscosity and yield stress of magnetic fluid applied to low temperature magnetic fluid sealScientific Reports · 2025
- Magnetic-Field-Controlled Thermohydrodynamic Behavior of Fe3O4/SWCNT Hybrid Ferrofluid in a Cavity with a Rotatable Elliptical BarrierMagnetochemistry · 2026
- Interfacial instability and failure mechanisms of ferrofluid seals in liquid environments: A ternary phase-field ferrohydrodynamic studyPhysics of Fluids · 2026
- Study on pumping characteristics of ferrofluid micropumps under magnetic field drive and interface instability couplingJournal of Physics: Conference Series · 2026
- Study on Influence Law and Mechanism of Rheological Properties of High-Viscosity Fluoroether Oil-Based FerrofluidsMagnetochemistry · 2025