Journal of Physics: Conference Series

Mechanism and causes of ammonium chloride crystallization in the tail flue of a circulating fluidized bed boiler

Qilong Zhang, Tianyu Liu, Yufeng Yan, Can Zhou

Key points

From the paper's conclusion
  • Meanwhile, the excessively high air leakage rate of the air preheater (reaching 40.680%) led to a low operating flue gas temperature of the dust collector, exacerbating the occurrence of ammonium chloride crystallization.

Abstract

Based on the Gibbs free energy of the ammonium chloride crystallization reaction and the principle of corresponding states, a prediction model for the crystallization temperature of ammonium chloride was established. The calculation based on this model shows that under the conditions of HCl concentration of 52.25 mg/m 3 and ammonia slip concentration of 151.37 mg/m 3 (standard dry, 6% O 2 ), the crystallization temperature of ammonium chloride is 121°C. This temperature is higher than the dust collector’s operating flue gas temperature of 117°C and is the main cause of ammonium chloride crystallization. The main factor for the increase in ammonia slip is that the residence time of NH 3 within the denitration reaction temperature has decreased from 5.6 seconds to 0.6 seconds, resulting in incomplete NH 3 reaction. Under these conditions, the reduction in denitrification efficiency leads to an increase in ammonia injection volume (the actual NH 3 /NO molar ratio is 2.23-9.12), which in turn intensifies ammonia slip. Meanwhile, the excessively high air leakage rate of the air preheater (reaching 40.680%) led to a low operating flue gas temperature of the dust collector, exacerbating the occurrence of ammonium chloride crystallization.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers