Journal of Physics: Conference Series

Fracture performance and fatigue life prediction of X80 pipeline steel weld joint based on strain energy

Wanpeng Tian, Lun Tang

Key points

From the paper's conclusion
  • An energy-based fatigue life prediction model taking inelastic strain energy density as the damage parameter was established.

Abstract

Aiming at embrittlement and low-cycle fatigue failure of X80 pipeline steel welded joints under low-temperature service conditions, quasi-static fracture toughness tests were performed by the single-specimen unloading compliance method, and J-resistance curves (J-∆a curves) of base metal (BM), weld metal (WM), and heat-affected zone (HAZ) were obtained. The average fracture toughness values of the three regions are 282.10 MPa·m 1/2 , 278.38 MPa·m 1/2 , and 269.23 MPa·m 1/2 , respectively. An energy-based fatigue life prediction model taking inelastic strain energy density as the damage parameter was established. This research provides theoretical support for structural integrity evaluation of X80 pipeline girth weld.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers