Journal of Physics: Conference Series

Degradation of silicone rubber for capacitors sealing application of thermal ageing

Yajun Qiao, Huan Pan, Yun Liu, Zibo Xu

Key points

From the paper's conclusion
  • In this paper, accelerated thermal ageing tests were conducted on sealing silicone rubber for capacitors at 105°C for up to 1500 h, to systematically investigate the degradation mechanism of silicone rubber for sealing application.

Abstract

In this paper, accelerated thermal ageing tests were conducted on sealing silicone rubber for capacitors at 105°C for up to 1500 h, to systematically investigate the degradation mechanism of silicone rubber for sealing application. The rubber samples were aged both in the impregnation fluid and in the air. Microstructural deterioration was observed as increased surface roughness and internal porosity. As for the mechanical properties, the rising hardness and compression deformation were exhibited, and the increment in the oil-impregnated samples was approximately one-third of that of the non-impregnated samples throughout the ageing process. The physical crosslinking density decreased sharply at the initial stage and then levelled off, while the chemical crosslinking density continuously increased; the total crosslinking density went up rapidly at first and then slowed down. The penetration of the impregnating agent significantly suppressed the accumulation of permanent deformation, thereby effectively improving the sealing reliability at high temperatures.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers