CFD simulation and experimental study on melt pool behavior and nitrogen porosity defects of high-nitrogen steel fabricated by LPBF and LDED
Haining Liu, Fajia Li, Kun Yang, Jitao Fang
Key points
From the paper's conclusion- Consequently, LDED fabrication leads to a decreased nitrogen retention of 0.381 wt.% and an elevated porosity of 0.61%.
Abstract
High-nitrogen steel (HNS) is a promising advanced structural material with exceptional strength and corrosion resistance, but its high work-hardening rate poses great challenges to conventional machining and forming processes. Laser-based additive manufacturing presents a transformative solution for the near-net-shape production of intricate HNS geometries, while nitrogen outgassing and resultant pore defects remain critical bottlenecks that degrade structural integrity. In this work, three-dimensional computational fluid dynamics (CFD) models are established for both LPBF and LDED processes. Combined with single-track experiments using identical pre-alloyed HNS powder, the thermal-fluid behavior of melt pools, nitrogen retention characteristics, and pore formation mechanisms are comparatively investigated. The simulated results aligned closely with the experimental data, maintaining a melt pool width error of less than 10%. Quantitative analysis reveals that the cooling rate of LPBF reaches 5.83×10 6 K/s, which is roughly three orders of magnitude faster than the cooling rate observed in LDED. The ultra-rapid solidification effectively suppresses nitrogen bubble nucleation and escape, achieving a retained nitrogen content of 0.413 wt.% and an ultra-low porosity of 0.27% with an average pore diameter of 9.22 μm. By contrast, the larger melt pool and longer liquid lifetime in LDED provide sufficient kinetic conditions for nitrogen outgassing. Consequently, LDED fabrication leads to a decreased nitrogen retention of 0.381 wt.% and an elevated porosity of 0.61%. Ultimately, this research elucidates the intrinsic relationship between defect evolution and melt pool thermodynamics, offering a foundational framework for optimizing process parameters in the additive manufacturing of HNS parts.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Review of the laser powder bed fusion of nitinol: Defect formation and predictionMaterials Today Advances · 2026
- Laser directed energy deposition of nickel-based superalloy: A numerical investigation of melt pool morphology and thermal evolutionJournal of Materials Research and Technology · 2026
- Plasma nitriding of additively manufactured 316L austenitic stainless steel produced by laser power bed fusion and metal binder jettingJournal of Materials Research and Technology · 2026
- Plasma Immersion Ion Implantation of AISI 316L Stainless Steel Parts Manufactured by Laser Powder Bed FusionJournal of Materials Engineering and Performance · 2026
- A versatile miniature laser powder bed fusion setup for in situ observations of keyhole and phase transformation dynamics via high-speed synchrotron imaging and diffractionReview of Scientific Instruments · 2026
- Entropy-driven densification of medium-entropy alloys with laser powder bed fusion.Nature communications · 2026