Journal of Physics: Conference Series
Evaluation of polycrystalline diamond bulk brazed onto WC-Co substrate through tungsten coating in air
Rui Chang
Key points
From the paper's conclusion- With the aid of the tungsten (W) coating, brazing the polycrystalline diamond (PCD) bulk onto the WC-Co substrate in air was achieved.
Abstract
With the aid of the tungsten (W) coating, brazing the polycrystalline diamond (PCD) bulk onto the WC-Co substrate in air was achieved. The W coating on the PCD was prepared by treating a mixture of PCD bulks and W powders at 950 ºC for 3 h in an SPS system. The coating consisted of WC, Si 2 W, and W phases, which was ~5 μm in thickness. In the prepared polycrystalline diamond composite, both of the interfaces between the brazing alloy and the W-coated PCD bulk or the WC-Co substrate were chemically bonded. The maximum shear strength between the W-coated PCD bulk and the WC-Co substrate was 87.8 MPa, which was achieved at 750 ºC for 13 s.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effects of particle size distribution of W-coated diamond particles on the properties of diamond/Al compositesJournal of Physics: Conference Series · 2026
- Effect of cobalt content and nickel interlayer on the bonding strength and properties of LCS\WC–Co via PM techniqueScientific Reports · 2026
- The Effect of De-Cobalt Pretreatment of PDC on the Deposition of Diamond CoatingsCoatings · 2026
- Comparative study on the morphology and tribological behaviour of Co/WS₂ , Co/WC, and hybrid Co/WC–WS₂ composite coatingsTransactions of the IMF · 2026
- Surface modification of hard diamond particles with Cu-Mo2C double layer coating and its application in thermal conductive compositesDiamond and Related Materials · 2025
- Enhanced interfacial strength and cutting performance of Fe-based diamond composites via Ti-coating induced interfacial optimizationJournal of Materials Research and Technology · 2026