Micro-trench measurement of selective boron deposition during boron powder dropper operation in DIII-D
Shota Abe, Florian Effenberg, Alessandro Bortolon, Igor Bykov, Jun Ren, Dmitry L Rudakov, Adam G McLean, Ryan Hood,
Key points
From the paper's conclusion- The selective boron (B) deposition rate is reported as measured using the micro-trench method in the DIII-D divertor during deuterium (D) H-mode outer strike point (OSP) sweeping plasma discharges with B powder injection via the impurity powder dropper (IPD).
Abstract
The selective boron (B) deposition rate is reported as measured using the micro-trench method in the DIII-D divertor during deuterium (D) H-mode outer strike point (OSP) sweeping plasma discharges with B powder injection via the impurity powder dropper (IPD). The selective deposition is defined as a result of B deposition and impurity sputtering (deposited B sputtered by B ions or other impurity ion species) in a micro-scale region geometrically shadowed from direct fuel/D+ ion bombardment. To perform this work, micro-trenches 32 µm × 32 µm × 4 µm deep were fabricated on a single-crystal silicon sample. The sample was exposed to DIII-D H-mode “cleaning” plasma discharges with D fueling and OSP sweeping via the Divertor Material Evaluation System (DiMES). The IPD injected B powder at rates of 5-20 mg/s during 2-5 s of H-mode plasmas in multiple discharges, adding up to 0.4 g injected in total. Injected B powders were ablated, ionized, and transported to PFC surfaces. Post-mortem analysis revealed that impurity deposition concentrated in a D+ ion shadowed area on the micro-trench floor, while no B deposition was observed outside of the micro-trench, which implied that net impurity deposition can be significantly enhanced by rough micro-structures on PFC surfaces, i.e., selective deposition. An energy-dispersive X-ray spectroscopy (EDS) analysis detected impurity deposition containing B, carbon, oxygen, and silicon. Combining the impurity deposition height profile measured by atomic force microscopy and the relative B concentration profiles measured by EDS, we determined the selective B deposition thickness of ~25 nm in the diverter region. The measured B deposition thickness agreed with a mass balance analysis to within half the magnitude when the B impurity flux was assumed to be concentrated near the OSP, as predicted by a real-time wall conditioning model developed to optimize IPD operations of advanced fusion reactors.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- First divertor exposure experiments of a renewable boron pebble aggregate in DIII-DNuclear Fusion · 2026
- Analysis of Solid Boron Injection for ITERarXiv · 2026
- A study of the influence of prolonged baking on deuterium depth distribution and release in JET ILW componentsNuclear Fusion · 2026
- Self-consistent integrated three-stage modeling of material erosion, migration, and surface evolution in fusion devicesPhysics of Plasmas · 2026
- TiO₂-Bi₂O₃ bimetallic oxide nanocomposite coatings for enhanced ignition and combustion of boron-based energetic materialsCombustion and Flame · 2025
- Structural effects of boron doping in diamond crystals for gamma-ray light-source applications: Insights from molecular dynamics simulationsDiamond and Related Materials · 2026