Smart Materials and Structures

Wire diameter as a key design variable for martensite transformation thermodynamics, kinetics, and mechanics in thin cold-drawn Ti49.6Ni45.4Cu5 wires

Timofey Chekalkin, Ji-Hoon Kang, Alex Volinsky, Aleksandr Grenaderov, Marina Kandaurova, Tatiana Sablina

Key points

From the paper's conclusion
  • XRD line-profile analysis indicated that the coherently scattering domain size increased from 5.9 to 14.7 nm with diameter, with the highest microstrain in the 25 µm wire.

Abstract

The effect of wire diameter on martensitic transformation behavior, microstructure, and room-temperature mechanical response was studied in Ti49.6Ni45.4Cu5 (at.%) wires with diameters of 25, 40, and 100 µm. The wires were produced by multi-pass cold drawing with a common final sizing reduction and annealed at 450 °C for 1 min. They were characterized by differential scanning calorimetry (DSC), two-cycle tensile testing, SEM-EDS, room-temperature XRD, and TEM/STEM-EDS. All wires showed a single-stage B2B19′ transformation, and Mf >22 °C, so deformation occurred predominantly within thermally formed martensite. Ms increased from 42.4 to 49.6 °C as the diameter decreased from 100 to 25 µm. A surface-energy penalty is too small and of the wrong sign to explain this trend, and defect- and surface-assisted nucleation is proposed instead. The transforming fraction was 0.8 and 0.83 for the 25 and 40 µm wires but only 0.37 for the 100 µm wire. XRD line-profile analysis indicated that the coherently scattering domain size increased from 5.9 to 14.7 nm with diameter, with the highest microstrain in the 25 µm wire. TEM/STEM-EDS of wire interiors revealed chemically equivalent, homogeneous matrices free of precipitates and second phases, with a deformed, incompletely recovered substructure. The deficit in fT for the 100 µm wire may reflect heterogeneous defect or residual-stress distributions, potentially including a less-transformable interior volume; this interpretation remains hypothetical because radial structural gradients and recrystallization fractions were not measured. The 25 µm wire had the lowest first-cycle residual strain but fractured at the lowest stress (≈980 MPa) and strain in the second cycle; surface-initiated fracture is proposed as a hypothesis. The four analytical relationships are reported as descriptive fits to the three diameters studied. The diameter trends themselves are experimental observations; the mechanisms proposed to explain them, including defect- and surface-assisted nucleation and a less transformable interior volume

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Wire diameter as a key design variable for martensite transformation thermodynamics, kinetics, and mechanics in thin cold-drawn Ti49.6Ni45.4Cu5 wires — Science Skim