From the paper's conclusion- Experimental validation using five powder groups (SMD ranging from 2.530 to 3.607 μm) demonstrates that the favorable powder morphology range occurs at SMD of 2.500–2.700 μm with D99/D10 < 7 under the processing conditions investigated in this study , arising from the competing effects of magnetic alignment efficiency (dominated by agglomeration at fine end) and mechanical retention efficiency (do
Abstract
The morphological characteristics of Nd-Fe-B powders critically determine the packing behavior, stress transmission, and final magnetic properties during the orientation compaction process. However, direct numerical simulation of the coupled magnetic-mechanical alignment remains computationally prohibitive and physically challenging. This study decouples the problem by employing Discrete Element Method (DEM) simulations to specifically investigate the mechanical-induced de-orientation mechanisms during the pressing stage, while treating the DEM particles as scale-up agglomerates with rigorous dimensionless number similarity analysis to maintain physical consistency with real powder systems. The Hysteretic Spring contact model was adopted to capture the elastoplastic deformation behavior of metallic agglomerates, with model parameters calibrated via angle-of-repose experiments (optimal rolling friction coefficient: 0.1226, simulation-experiment deviation < 2%). Dimensionless analysis confirms that the simulated agglomerates match real powders in terms of packing fraction and effective internal friction angle, validating the scale-up approach. Simulation results reveal that reducing the agglomerate size from 2.8 mm to 2.0 mm (with correspondingly narrower size distribution) decreases green compact porosity by 12.13%, average compressive stress by 31.44%, and average torque by 50.20%. Advanced micromechanical analyses demonstrate that finer, uniformly distributed powders exhibit more gradual coordination number evolution during compaction, avoiding abrupt stress concentration and associated shear-induced rotation. The simulation validity was confirmed through Huang Peiyun's double-logarithmic pressing equation with correlation coefficients R² approaching unity. Experimental validation using five powder groups (SMD ranging from 2.530 to 3.607 μm) demonstrates that the favorable powder morphology range occurs at SMD of 2.500–2.700 μm with D99/D10 < 7 under the processing conditions investigated in this study , arising from the competing effects of magnetic alignment efficiency (dominated by agglomeration at fine end) and mechanical retention efficiency (dominated by stress concentration at coarse end).
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Linkage between process-induced microstructure and magnetic property of Nd-Fe-B permanent magnets additively manufactured by laser powder bed fusionMaterials & Design · 2025
- A Review of the Discrete Element Method (DEM) Simulation of Mineral Comminution Processes: Part I. Theoretical DevelopmentsMetaResource · 2025
- Numerical Simulation Study of Multiscale Magnetization Behavior in Magnetic MaterialsJournal of Physics: Conference Series · 2026
- Investigation on the material extrusion additive manufacturing of unalloyed magnetic steelRapid Prototyping Journal · 2026
- Phase field study of exchange coupling of hard/soft ferrite on magnetic permeabilityJournal of Applied Physics · 2026
- Advances in discrete element modeling of rock fracture for next-generation comminution modelsComputational Particle Mechanics · 2025