From the paper's conclusion- The results show that spherulite refinement markedly increases the characteristic DC breakdown field and reduces volume conductivity, while tensile testing further reveals concurrent improvements in tensile strength and elongation at break.
Abstract
Polypropylene (PP) is a promising recyclable insulating material for next-generation high-voltage direct-current (HVDC) cables, owing to its melt recyclability, thermal stability and favourable DC dielectric performance. While cooling-rate regulation is known to modify PP crystallization morphology and space-charge behaviour, the microstructural mechanism by which spherulite size simultaneously governs charge transport, electrical breakdown and mechanical fracture remains insufficiently understood. In this work, PP films with varying spherulite sizes were prepared by controlling the cooling rate during non-isothermal crystallization. DC breakdown strength, volume conductivity and tensile properties were characterized. Local trap parameters in crystalline interiors and interspherulitic amorphous boundaries were extracted in situ using atomic force microscopy (AFM)-assisted nanoscale isothermal surface-potential decay, and were incorporated into an electrical breakdown coupled with molecular displacement model based on two-dimensional Voronoi morphology. The results show that spherulite refinement markedly increases the characteristic DC breakdown field and reduces volume conductivity, while tensile testing further reveals concurrent improvements in tensile strength and elongation at break. Local measurements reveal that amorphous boundaries have a lower deep-trap density than spherulite interiors, rendering them relatively high-conductivity regions. Nevertheless, macroscopic conductivity is governed not by local conductivity alone, but by the long-range connectivity of these amorphous pathways. Large spherulites form continuous boundary networks, which promote charge migration, field distortion and electron-energy accumulation. In contrast, refined spherulites divide the amorphous phase into shorter and more tortuous pathways, effectively suppressing continuous charge transport, molecular-chain displacement and through-crack propagation. This topology-induced confinement mechanism accounts for the concurrent improvement in DC insulation strength and mechanical toughness of PP.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Small Strain-Induced Abrupt Drop in the Electrical Breakdown Strength of Polypropylene InsulationNano Letters · 2025
- Mesoscale Heterophase Structural Design in Polypropylene: A Strategy for Dielectric Enhancement via Charge and Field ModulationACS Applied Polymer Materials · 2026
- Aggregation-State Tailored Insulation Robustness by Spherulite Size Control in Semicrystalline Poly(vinylidene fluoride) FilmACS Materials Letters · 2025
- Relationships of Multiphase Structure with Flexibility and DC Insulation Performance in Impact-Resistant Polypropylene Copolymers.Polymers · 2026
- Melt Grafting of Geometry‐Tailored Voltage Stabilizers for High‐Performance Polypropylene InsulationAdvanced Functional Materials · 2025
- Enhancing the Comprehensive Properties of Polypropylene Films via Organic–Inorganic Interfacial Molecular EngineeringPolymer Engineering & Science · 2026