  • The results indicated that during the RAM process, the mechanical, thermal, and electrostatic stimuli experienced by the cast PBX simulant were of the same magnitude as those under traditional processes, such as vertical kneading, with no significant differences observed.

Abstract

An online measurement device for mechanical–thermal–electrostatic stimuli was established to address the lack of process stimulus parameters for safety evaluation when applying the novel Resonance Acoustic Mixing (RAM) technology to prepare cast polymer bonded explosive (PBX). Using a cast PBX simulant as the target material, the impact force, temperature, and electrostatic voltage experienced by the mixture during the mixing process were measured. These values were compared with the stimulus levels of typical traditional processes in energetic materials preparation to analyze the stimulus characteristics and their influence on the RAM process. The results indicated that during the RAM process, the mechanical, thermal, and electrostatic stimuli experienced by the cast PBX simulant were of the same magnitude as those under traditional processes, such as vertical kneading, with no significant differences observed. Mechanical stimuli showed a linear positive correlation with acceleration, and formulations with lower solid content experienced greater mechanical stimuli, reaching a magnitude of ∼500 kPa. The temperature rise due to thermal stimuli was related to the mixing time—longer mixing times before reaching thermal equilibrium resulted in higher temperatures. The heat generation rate was primarily influenced by acceleration and the state of the material, with the maximum rate ranging between 0.04 °C/s and 0.1 °C/s across different formulations. When a metal conductive container with proper grounding was used, the electrostatic voltage during mixing was ∼50 V. In contrast, under insulating conditions, the electrostatic voltage of powdered materials could reach up to 1000 V.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Influence factors and patterns of stimuli in the resonance acoustic mixing (RAM) process of pourable polymer bonded explosive (PBX) simulants — Science Skim