Influence of basicity on techno-economic indicators and metallurgical properties of low-silicon sinter
Tan Peilong, Zhang Yu, Zhang Jianliang, Liu Zhengjian, Wang Yaozu
Key points
From the paper's conclusion- Comprehensively considering the techno-economic indicators and metallurgical properties, especially the critical importance of softening-melting-dripping performance for blast furnace stability, the optimum basicity for low-silicon sinter is determined to be 2.0.
Abstract
To clarify the influence of basicity on the techno-economic indicators and metallurgical properties of low-silicon sinter (SiO 2 content of 4.96–5.00%), six sintering pot tests were conducted with basicity (R) levels of 1.8, 1.9, 2.0, 2.1, 2.2, and 2.3, using iron ore fines from Meishan Steel as raw materials. The vertical sintering speed, tumble strength, product size distribution, utilization coefficient, reducibility (RI), low-temperature reduction disintegration index (RDI +3.15 ), softening-melting-dripping performance, liquid phase formation, and mineral phase evolution were systematically analyzed. The results show that as the basicity increases from 1.8 to 2.3, the vertical sintering speed first increases and then stabilizes, reaching a maximum of 20.59 mm/min at R = 2.2. Both the tumble strength and RDI +3.15 peak at R = 2.1, with values of 70.67% and 61.25%, respectively. The utilization coefficient is highest at R = 2.0 (1.13 t·m −2 h −1 ). The softening-melting-dripping performance (S-value) deteriorates sharply when the basicity exceeds 2.0: it is 264 kPa·°C at R = 2.0, rises to 341 kPa·°C at R = 2.1, and exceeds 353 kPa·°C at R ≥ 2.2. Liquid phase calculation and mineral phase observation indicate that increasing basicity promotes the formation of silico-ferrite of calcium and aluminum (SFCA), which enhances strength and reducibility. However, excessive basicity (≥2.2) leads to the degeneration of the SFCA crystal morphology into a granular form and the formation of dicalcium silicate (C 2 S), generating microcracks that deteriorate the product size distribution and melting-dripping properties. Comprehensively considering the techno-economic indicators and metallurgical properties, especially the critical importance of softening-melting-dripping performance for blast furnace stability, the optimum basicity for low-silicon sinter is determined to be 2.0.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of the Hematite/Limonite Ratio on Sinter Properties and the Underlying Microscopic MechanismMetals · 2026
- Thermodynamic analysis of Silico‑Ferrite of Calcium and Aluminum (SFCA) formation via reaction pathways during iron ore sintering and its limitations: Considerations for energy efficiency in sustainable metallurgyJournal of Materials Science: Metallurgy · 2026
- Fundamental Analysis of Sinter Solid Structure: Implications of Mineral Associations for Understanding Industrial Iron Ore Sinter FormationMinerals · 2026
- Effect of By-Product-Derived Low-Melting-Point Additive on Mineralogical and Metallurgical Properties of Iron Ore SinterMinerals · 2026
- A dilatometric study of phase transformation for a Fe–C–Ni–Mo(−Si) sustainable advanced high strength steelMaterials & Design · 2026
- Revealing contradictory reduction behavior in shaft furnaces at increasing H2 contents: Combined roles of thermodynamic equilibrium differences and gas flow rateFuel · 2026