Hardness gradients and galvanic corrosion behaviour of hybrid laser powder bed fusion-Al10SiMg on wrought 6061 aluminium substrates
Ngeleshi Michel Kibambe, Lerato Semetse, Mpinda Bob Mampuya, Mosima Edith Maja, Samson Dare Oguntuyi, Velile Vilane, Peter Apata Olubambi
Key points
From the paper's conclusion- This study investigated the microstructural integrity, mechanical gradients, and electrochemical stability of hybrid components fabricated by depositing AlSi10Mg via Laser Powder Bed Fusion (LPBF) onto a wrought 6061 aluminium alloy substrate.
Abstract
This study investigated the microstructural integrity, mechanical gradients, and electrochemical stability of hybrid components fabricated by depositing AlSi10Mg via Laser Powder Bed Fusion (LPBF) onto a wrought 6061 aluminium alloy substrate. Microhardness profiling revealed a distinct mechanical discontinuity across the assembly: the refined structure of the LPBF-AlSi10Mg achieved an increased surface hardness of 130 ± 5 HV, while the 6061-substrate maintained a base hardness of 91 ± 4 HV, and the interface exhibits a localized “softening valley” which reduced the hardness to 80 ± 4 HV. This interfacial weakening was attributed to the thermal cycles of the LPBF process, which induce precipitate dissolution within the heat-affected zone. Electrochemical evaluations (OCP, PDP, and EIS) in a 3.5 wt.% NaCl environment demonstrated a strong micro-galvanic relationship where the hybrid component exhibited high corrosion activity, which was driven by the potential mismatch between the active (anodic) LPBF layer and the comparatively more noble (cathodic) substrate. An accelerated 7-day immersion testing in an acidic environment confirmed that degradation was localized at the interface, while 3D Atomic Force Microscopy (AFM) reveals catastrophic material loss exceeding 10 μm. post-corrosion analyses conducted via scanning electron microscopy (SEM) and Raman spectroscopy identified that during chemical dissolution, the interface and the fish-scale melt pool boundaries were preferentially attacked, which encouraged microcrack initiation points. These findings highlighted that while hybrid additive manufacturing provides strong metallurgical bonding, the interfacial thermal softening and micro-galvanic susceptibility still have critical constraints for the long-term structural integrity of aluminium hybrid systems.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of Friction Stir Welding and Post-Weld Aging on Corrosion Behavior of LPBF A20X AlloyMetals · 2026
- Microstructure-driven formation of a chemically graded corrosion layer in PBF-LB/M fabricated dual-phase Mg–8Li–0.5Ca wt.% ultralight alloyJournal of Magnesium and Alloys · 2026
- The Corrosion Properties of Al-Cu-Mg Alloy Fabricated via Additive Friction Stir Deposition.Materials (Basel, Switzerland) · 2026
- Investigation of Solid Particle Erosion Wear Behavior of Additively Manufactured AlSi10Mg Alloys Under Cryogenic ConditionsJournal of Tribology · 2026
- The influence of part height on the properties and microstructure of AlSi7Mg produced by laser powder bed fusionThe International Journal of Advanced Manufacturing Technology · 2026
- Cavitation erosion-corrosion properties of as-cast NiTi and LPBF NiTi in 3.5 wt% NaCl solution: A comparison investigation.Ultrasonics sonochemistry · 2026