Impact of polycrystalline silicon contact layers on the device performance of TBC solar cells
Zhibin Jiang, Fen Yang, Yi Xie, Taihong Xie, Lili Wu, Xia Hao, Guanggen Zeng, Zhengguo Yuan,
Key points
From the paper's conclusion- The study therefore presents the Quokka3 results as experimentally constrained process guidance and identifies which predictions still require targeted production-line validation.
Abstract
Tunnel-oxide passivated back-contact (TBC) solar cells combine TOPCon-type passivating contacts with an interdigitated rear-contact architecture. Their efficiency is controlled by mutually coupled optical absorption, lateral transport, and recombination losses in the rear p-type and n-type poly-Si contacts. In this work, Quokka3 was used as a three-dimensional device-level sensitivity tool constrained by a production-line reference device, wavelength-dependent optical-generation profiles, electrochemical capacitance-voltage (ECV) active-doping measurements, and factory process windows. The purpose of the simulations was not to reproduce every production batch, but to separate loss mechanisms that cannot be independently varied in finished cells. Thickness scans show that parasitic absorption in n-type poly-Si is the dominant thickness-related limitation to J sc , whereas p-type poly-Si exhibits a broader trade-off between optical loss and metal-contact shielding. With p-type poly-Si at Rsheet = 100 Ohm sq −1 and n-type poly-Si fixed at 3 × 10 20 cm −3 and 340 nm, the preferred p-type active-doping range is 4 × 10 19 –6 × 10 19 cm −3 , giving simulated efficiencies of 27.109–27.112% under the stated boundary conditions. Increasing n-type poly-Si doping progressively reduces J sc through free-carrier absorption and Auger recombination unless the loss is compensated by lower contact resistance. ECV confirms a pronounced boron diffusion tail in p-type poly-Si and a box-like phosphorus profile in n-type poly-Si, providing material-level constraints for the simulation inputs. Production data provide trend-level validation: stable p-type poly-Si processing occurs near 290–300 nm and 115–135 Ohm sq −1 , whereas an n-type poly-Si layer of approximately 340 nm and 27 Ohm sq −1 remains the robust industrial condition. The study therefore presents the Quokka3 results as experimentally constrained process guidance and identifies which predictions still require targeted production-line validation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Passivating pinholes for large-area and high-efficiency silicon solar cells with tunnel oxide passivated contactNature Communications · 2026
- Numerical investigation of perovskite solar cells: impact of TCO selection and absorber layer properties using SCAPS-1DPhysica Scripta · 2026
- TOPCon-based bottom cells for perovskite/silicon tandem solar cellsJoule · 2026
- Fully‐Textured Perovskite/Silicon Tandem Solar Cells Exceeding 30% Efficiency on Both Side Tunnel Oxide Passivating Contacted Bottom CellsSolar RRL · 2025
- Thermal Stability of Nitrogen-Doped Tunnel Oxide Passivating Contact Structures for Future Chalcogenide/Silicon Tandem Solar Cells.ACS applied materials & interfaces · 2026
- Conductivity-Engineered Polymeric Rear Contacts for Bifacial Sb2(S,Se)3 Solar Cells and 4T Tandem Photovoltaics.Advanced materials (Deerfield Beach, Fla.) · 2026