Interfacial defect sensitivity and failure-site competition in biomimetic mushroom-shaped micropillar adhesion.
Zirui Ling, Zhihua Ning, Yue Li, Qiang Wen
Key Laboratory of Marine Civil Engineering Materials and Structures, Ministry of Education of China, School of Mechanics and Construction Engineering, Jinan University, Guangzhou, China. tningzhihua@jnu.edu.cn.
Key points
From the paper's conclusion- Here, we combine cohesive-zone-model-based simulations with in situ frustrated total internal reflection imaging to establish a mechanics-based framework for quantifying defect sensitivity in mushroom-shaped micropillar adhesion.
Abstract
Bioinspired mushroom-shaped micropillars are representative structural units of dry adhesive materials, yet their adhesion reliability is highly susceptible to interfacial defects. Although micropillar geometry has been widely optimized under ideal contact conditions, how defect topology governs debonding pathways, strength degradation and defect tolerance remains insufficiently understood. Here, we combine cohesive-zone-model-based simulations with in situ frustrated total internal reflection imaging to establish a mechanics-based framework for quantifying defect sensitivity in mushroom-shaped micropillar adhesion. We show that defects reduce adhesion not simply by removing contact area, but by initiating local debonding at defect boundaries, thereby altering the pathway of interfacial peeling and global failure. Cap thickness is identified as a key structural parameter: thicker caps, with increased bending stiffness, exhibit improved tolerance to central defects by reducing the sensitivity of global debonding to localized defects. Defect location further controls interfacial peeling. Edge-connected defects readily activate debonding near the free boundary and substantially reduce the pull-off force, whereas small central defects have limited influence, forming a defect-tolerant zone in the central region (r/R ≤ 0.4). Defect geometry also plays an important role. For sector-shaped edge defects, radial penetration depth is a more critical geometric descriptor than circumferential length, because deeper penetration into the load-bearing contact region produces more severe degradation of pull-off force. Under dual-defect conditions, adhesion degradation does not follow linear area superposition. Instead, global failure is controlled by the defect that first reaches the critical debonding condition, with sufficiently large or deeply penetrating edge defects more likely to dominate failure. These findings reveal the mechanical link between defect geometry, structural compliance, and global adhesive failure, providing a basis for the defect-tolerant design of robust bioinspired dry adhesives.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Impact-Induced Adhesion Degradation in Gecko-Inspired Fibrillar Adhesive Units.Bioinspiration & biomimetics · 2026
- A Scalable Double-Sided Wet Etching Strategy for Large-Area Mushroom-Shaped Bionic Adhesives.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026
- Shape Memory Polymer-Based Switchable Bioinspired Microstructured Dry Adhesives.Nano letters · 2026
- Trapezoidal Microstructure-Mediated Antagonistic Regulation of Liquid-Bridge Capillary Force and Wetting Stability.Langmuir : the ACS journal of surfaces and colloids · 2026
- Mode Transition and Cohesive Failure during Ice Debonding from Microstructured Surfaces.Langmuir : the ACS journal of surfaces and colloids · 2026
- Deterministic Noncontact Release and Transfer Through Programmable Interfacial Stress Reconfiguration.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026