Effect of calcination time on the NH3-SCR performance of 8Fe2O3-5CeO2-40MnO2/TiO2 catalysts.
Yu Chen, Yuming Yang, Xue Bian, Jiaqi Li, Xuewen Mu, Zhongshuai Jia, Zhicheng Wang, Bin Zhang,
Baogang Group Mining Research Institute Baotou 014030 China yangyuming98@163.com. · School of Metallurgy, Northeastern University Shenyang 110819 China.
Key points
From the paper's conclusion- Under the conditions examined, calcination at 400 °C for 4 h provided the most suitable balance between physicochemical properties and catalytic performance.
Abstract
Low-temperature NH3-SCR catalysts can reduce the energy demand associated with reheating flue gas after desulfurization and particulate removal. In this work, 8Fe2O3-5CeO2-40MnO2/TiO2 catalysts were prepared by co-precipitation and calcined at 400 °C for different dwell times. Shorter treatment left the pore network and exposure of the active components insufficiently developed, whereas further extension of the dwell time provided an additional improvement in catalytic performance. However, extending the dwell time to 5 h provided no further catalytic benefit and was accompanied by renewed aggregation. Calcination for 4 h gave the best overall NH3-SCR response: NO conversion exceeded 80% from 115 to 425 °C and 90% from 129 to 390 °C, with a maximum of (99.17 ± 0.6)%, while N2 selectivity remained close to 100% below 225 °C. At 200 °C, the sample retained stabilized NO conversions of (84.8 ± 0.7)% under 60 ppm SO2 and (81.6 ± 0.8)% under 60 ppm SO2 and 5 vol% H2O. The structural and surface analyses showed well-developed porosity, weaker aggregation, greater exposure of the active components, increased surface acidity and improved reducibility after 4 h. This catalyst also exhibited the lowest apparent activation energy of 55.78 kJ mol-1. Under the conditions examined, calcination at 400 °C for 4 h provided the most suitable balance between physicochemical properties and catalytic performance.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Calcination Temperature on the Structure and NH3-SCR Performance of 8Fe2O3-5CeO2-40MnO2/TiO2 CatalystsCatalysts · 2026
- Comparative Effects of Ce, Co, or W Dopants on the Catalytic Performance of FeMnTiOx Catalysts for Low-Temperature NH3-SCR of NO.Molecules (Basel, Switzerland) · 2026
- Unraveling the Poisoning Resistance Mechanism of an In Situ Fabricated SiO2/CoMnFe Layered Double Oxide Catalyst to NH3-SCR.ACS applied materials & interfaces · 2026
- Lattice-confined Ce-O-Mn pairs in anatase TiO2 for superior N2 selectivity during photo-assisted NH3-SCR deNOx.Journal of hazardous materials · 2026
- Ti doping-induced strain engineering boosts low-temperature NH3-SCR deNOx performance and H2O/SO2 resistance of Ce8MnOx.Nature communications · 2026
- Effect of Microwave Activation on the Activity of Multiphase Heterogeneous CuO/CuFe2O4 Mixed Catalysts for NH3-SCR of NO.ACS omega · 2026