New amide-functionalised extractants for the separation of Co(ii) from Ni(ii) and Mn(ii).
Korban Oosthuizen, Teagan Williams, Robert C Luckay
Stellenbosch University Private Bag X1, Matieland Stellenbosch 7600 South Africa rcluckay@sun.ac.za.
Key points
From the paper's conclusion- Amide-functionalised diamine extractants developed in this work demonstrate high Co(ii) extraction efficiencies, good selectivity over Ni(ii) and Mn(ii), and fast extraction kinetics under highly saline, moderately acidic conditions (10 M Cl-, 0.1 M HCl).
Abstract
This study investigates the use of compounds as solvent extraction agents, with particular emphasis on optimising extraction conditions to enhance both selectivity and efficiency. The separation of Co(ii) from Ni(ii) and Mn(ii)-containing solutions via metalate anion extraction represents a promising strategy for recycling NMC battery cathode materials. This approach exploits the pronounced differences in the tendency of these metals to form chlorido metalate anions in aqueous Cl- media. Under such conditions, Co(ii) exists in equilibrium between its hydrated cationic form and the doubly charged tetrachloridocobaltate anion (CoCl4 2-), whereas Ni(ii) and Mn(ii) form negligible amounts of anionic Cl- species. Amide-functionalised diamine extractants developed in this work demonstrate high Co(ii) extraction efficiencies, good selectivity over Ni(ii) and Mn(ii), and fast extraction kinetics under highly saline, moderately acidic conditions (10 M Cl-, 0.1 M HCl). Under optimal conditions (10 M Cl-, 0.1 M HCl) using 0.01 M extractant and 0.01 M of each metal ion (0.03 M total divalent metals), extractant L3 extracted 76% of Co(ii) in a single stage, with high selectivity over Ni(ii) (β Co/Ni = 70.2) and moderate separation from Mn(ii) (β Co/Mn = 19.9). Furthermore, Co(ii)/Ni(ii) selectivity can be fine-tuned by adjusting the aqueous phase acidity; above 0.01 M HCl, selectivity remains high for Co(ii), whereas reducing the HCl concentration below this threshold results in a significant increase in Ni(ii) co-extraction. Notably, the structurally inverted isomer L2 successfully lowers the high salinity requirement, achieving 41% Co(ii) extraction at a reduced Cl concentration of 6 M, compared to only 10% for its counterpart L4. Efficient, selective stripping of Co(ii) is achieved using 0.1 M HCl, yielding an average cobalt recovery of 95% over five continuous load-strip cycles while co-extracted Ni(ii) and Mn(ii) are preferentially retained in the organic phase, further enhancing final cobalt purity.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Highly selective and near-complete electrochemical recovery of cobalt and nickel from spent batteries through multifunctional deep eutectic solventEnergy storage materials · 2025
- Selective Electrodeposition of Cobalt from Lithium-Ion Battery Cathodes via Speciation Control and Surface-Modified Porous Electrodes.ACS nano · 2026
- Selective separation of Ni from Co and Mn in spent lithium-ion batteries using a novel tetramethylammonium chloride-based deep eutectic solventSustainable materials and technologies · 2025
- Synergistic Solvent Extraction of Ni, Co, and Mn from Ca/Mg-Containing Sulfate Solutions for Battery Metal RefiningIndustrial & Engineering Chemistry Research · 2026
- Direct Nickel Recovery From Spent NCM Lithium - Ion Batteries Enabled by Hydrophobic Sulfur - Donor Extractants.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Selective cobalt and nickel separation by bioacid-mediated electrowinningScience Advances · 2026