Tailoring the structural, optical and paramagnetic properties of GO-PVA-AgNW nanocomposites by gamma irradiation.
Mahammad Baghir Baghirov, Mustafa Muradov, Goncha Eyvazova, Zeynab Addayeva, Marjetka Conradi, Matjaz Malok, Hokman Mahmudov, Gasimov Eldar Kochari,
Nano Research Laboratory, Baku State University 23 Academik Zahid Khalilov Street Baku AZ1148 Azerbaijan bmbaghir@gmail.com. · Institute of Metals and Technology Lepi pot 11 1000 Ljubljana Slovenia.
Key points
From the paper's conclusion- In this study, GO-PVA-AgNW nanocomposite films were exposed to high-dose γ-irradiation (250, 500, and 1500 kGy) from a 60Co source, and the resulting morphological, structural, optical, thermal, and paramagnetic modifications were systematically investigated using scanning electron microscopy (SEM), X-ray diffraction (XRD), Raman spectroscopy, ultraviolet-visible (UV-vis) spectroscopy, thermogravi
Abstract
Graphene oxide (GO)-polyvinyl alcohol (PVA)-silver nanowire (AgNW) ternary nanocomposites are of increasing interest as radiation-resistant materials, yet their structural and physicochemical response under high absorbed gamma doses remains largely unexplored. In this study, GO-PVA-AgNW nanocomposite films were exposed to high-dose γ-irradiation (250, 500, and 1500 kGy) from a 60Co source, and the resulting morphological, structural, optical, thermal, and paramagnetic modifications were systematically investigated using scanning electron microscopy (SEM), X-ray diffraction (XRD), Raman spectroscopy, ultraviolet-visible (UV-vis) spectroscopy, thermogravimetric analysis (TGA), and electron paramagnetic resonance (EPR) spectroscopy. XRD and Raman analyses revealed a pronounced reduction in crystallite size (from 1.75 to 0.92 nm) accompanied by an increase in microstrain (from 0.115 to 0.217) and defect density with increasing dose. UV-vis spectroscopy showed a progressive red shift of the absorption edge and a decrease in the optical band gap from 5.07 (pristine) to 3.82 at 1500 kGy. TGA demonstrated enhanced thermal stability of the primary polymer backbone and an increase in residual carbonaceous content from 10.15% to 14.09%, indicating that crosslinking becomes the dominant process over chain scission at high absorbed doses. EPR measurements confirmed a dose-dependent increase in the concentration of carbon-centered π-radicals, together with a narrowing of the peak-to-peak linewidth and an evolution of the asymmetry factor toward unity, reflecting enhanced spin-exchange interactions and a more homogeneous radical distribution.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Dose-dependent structural and dielectric response of γ-irradiated PVA/GO/FeGaInS4 nanocomposite films.RSC advances · 2026
- Application insights on gamma irradiated PVA/TiO2 films: molecular structure, optical properties and DFT calculationsNuclear Instruments and Methods in Physics Research Section B Beam Interactions with Materials and Atoms · 2026
- The Effect of Gamma Irradiation on the Subsequent Thermal Reduction of Graphene Oxide Aerogel MonolithsHigh Energy Chemistry · 2026
- Effect of temperature and gamma irradiation on dielectric properties of FeGaInS₄ /PVA compositesRSC Advances · 2026
- Radiation-Induced Modification of Antioxidant-Active Biodegradable Starch-PVA Films: Effect of Phenolic Additive Structure and Nanofiller Reinforcement.Polymers · 2026
- Influence of oxygen ion irradiation on the chemical, structural, and morphological properties of poly(2,5-benzimidazole)/graphene oxide compositesPolymer Degradation and Stability · 2026