High dielectric performance with low losses in solution-grown CsPbBr3 single crystals revealed by impedance spectroscopy.
Maksym Pecherkin, Vasyl Mykhailovych, Matthias Gutmann, Mariia Mykhailovych, Aurelian Rotaru, Ion Soroceanu, Gheorghe Lucian Păşcut, Yuriy Khalavka,
Department of Chemistry and Food Expertise, YuriyFedkovych Chernivtsi National University 2, Kotsjubynskyi St. 58012 Chernivtsi Ukraine pecherkin.maksym@chnu.edu.ua. · Technology Transfer Center in Industry 4.0 and Smart Destinations & Department of Electrical Engineering and Computer Science, Stefan Cel Mare University of Suceava 720229 Suceava Romania.
Key points
From the paper's conclusion- The results indicate a high apparent permittivity combined with low high-frequency losses in solution-grown all-inorganic CsPbBr3 single crystals and provide reference dielectric parameters for the modelling of perovskite-based devices; they were obtained on a single crystal in a two-terminal configuration, so the effects of crystal thickness and surface leakage remain to be investigated.
Abstract
In this study, the dielectric and electrical properties of a solution-grown CsPbBr3 single crystal were investigated in an Au/CsPbBr3/Au device configuration using broadband impedance spectroscopy (0.1 Hz-1 MHz, in the dark at room temperature). The fully inorganic CsPbBr3 single crystal was grown by the antisolvent vapor-assisted crystallization method, yielding a well-defined rectangular crystal with dimensions of approximately 5 × 5 × 2 mm. At high frequency the crystal combines a high apparent permittivity, ε' ≈ 110 at 1 MHz (planar-capacitor approximation, single crystal thickness), with low dielectric losses: the loss tangent decreases from tan δ ≈ 0.38 at 1 kHz to below 10-2 above ≈2 × 105 Hz and reaches ≈2 × 10-4 at 1 MHz (the upper end of the measured range). Toward low frequencies, ε' increases to ≈2400 at 0.1 Hz, reflecting the contribution of slow polarization processes and interfacial charge accumulation. Electric modulus analysis reveals a dominant relaxation maximum at f max ≈ 610 Hz, corresponding to a relaxation time of τ ≈ 2.61 × 10-4 s. Additional Havriliak-Negami-type fitting confirms the non-Debye character of the dielectric relaxation, with distributed relaxation contributions associated with ionic/space-charge polarization and charge-transport-related processes. Equivalent-circuit analysis using two serially connected R‖CPE branches (the series resistance was found to be negligible) provides a phenomenological separation of higher-frequency bulk-related and low-frequency interfacial contributions and yields an apparent resistivity of ρ ≈ 4.4 × 108 Ω cm. The results indicate a high apparent permittivity combined with low high-frequency losses in solution-grown all-inorganic CsPbBr3 single crystals and provide reference dielectric parameters for the modelling of perovskite-based devices; they were obtained on a single crystal in a two-terminal configuration, so the effects of crystal thickness and surface leakage remain to be investigated.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Exploring Charge Transport, Trap States, and Activation Energy of High-Quality CsPbBr3 Single Crystal Grown by Inverse Temperature Crystallization for Photodetector Applications.ACS omega · 2026
- As‐Grown CsPbBr 3 Single Crystal With Atomically Smooth Surface Enabling High‐Performance X‐ray DetectionLaser & Photonics Reviews · 2026
- Submicron CsPbBr3 crystallites prepared through in situ moisture-driven decomposition of Cs4PbBr6 microcrystalsCommunications Chemistry · 2026
- Portable Dosimeter With Ultralow Detection Limit Enabled by Large Size Solution Grown Inorganic Perovskite Single CrystalAdvanced Materials · 2026
- Zero-Dimensional Lead-Free Perovskite Single Crystals for High-Performance Photodetection.Nanomaterials (Basel, Switzerland) · 2026
- A Review of Defect Formation Mechanisms, Their Impact on Radiation Detection Performance, and Defect Suppression Strategies in Melt-Grown CsPbBr3 Single CrystalsCrystals · 2026