Mitigating degradation in high-voltage LiNi0.5Mn1.5O4 cathodes via spray pyrolysis synthesis of single crystals with enhanced interfacial stability performance.
Daniele Callegari, Mauro Coduri, Umberto Anselmi Tamburini, Eliana Quartarone
Department of Chemistry, University of Pavia, Via Taramelli 16, Pavia 27100, Italy. daniele.callegari@unipv.it.
Key points
From the paper's conclusion- Herein, single crystal LiNi0.5Mn1.5O4 (LNMO) was synthesized via spray pyrolysis followed by subsequent annealing to achieve optimal electrochemical performance and superior cycling stability.
Abstract
The increasing demand for affordable and reliable energy storage has led to unprecedented interest in advanced battery technologies, particularly state-of-the-art lithium-ion (Li-ion) batteries. Consequently, research efforts have intensified significantly toward developing novel electrode materials. Among these, LiNi0.5Mn1.5O4 (LNMO) has been extensively studied as a promising cathode material owing to its high operating voltage, despite challenges associated with its conventional solid-state synthesis. Herein, single crystal LiNi0.5Mn1.5O4 (LNMO) was synthesized via spray pyrolysis followed by subsequent annealing to achieve optimal electrochemical performance and superior cycling stability. Spray pyrolysis serves as a versatile and scalable strategy suitable for industrial-scale production among the various synthesis and processing methods available for functional oxides. Following post-annealing, all materials exhibited a capacity retention of approximately 90% over 200 cycles at a 1C rate. Extended cycling stability over 1000 cycles at 1C was achieved for the optimal formulations, namely LNM_800°C_12h and LNM_850°C_12h, which consistently delivered specific discharge capacities exceeding 110 mAh g-1 with a capacity retention of 71%. In contrast, the commercial cathode benchmark underwent severe capacity degradation, retaining only 19% of its initial capacity by the end of testing. Furthermore, SEM micrographs and ICP analyses confirmed that the single crystal LNMO particles possess remarkable resistance to microcracking and significantly suppressed transition-metal leaching. This combination of exceptional electrochemical performance, morphological and structural stability, and enhanced resistance to transition-metal dissolution establishes single crystal LNMO as a highly competitive cathode material for next-generation Li-ion batteries.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Direct Synthesis of Single-Crystalline LiNi0.8Co0.1Mn0.1O2 Cathodes From Lithium-Containing Precursors via Spray Pyrolysis.Small science · 2026
- One‐Pot Spray Pyrolysis Fabrication of Multi‐Phase Lithium Manganese Oxide Microsphere Cathodes for Enhanced Lithium‐Ion Battery PerformanceEnergy & environment materials · 2026
- Fabrication of Homogeneous Nanometer-Thin Artificial CEI on LNMO by Suspension Coating of Niobate Nanosheets.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Decoupled Synthesis Pathway via Precursor Functionalization Stabilizes High-Voltage Nickel-Based Cathodes.Advanced materials (Deerfield Beach, Fla.) · 2026
- A General Spatial-Confinement Strategy for Atomic-Level Engineering of Single-Crystal Li-Rich Manganese-Based Oxides.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Highly Reversible Li-Insertion/Extraction in Octahedral Voids of LiNi0.5Mn1.5O4 Cathode With Restricted SnS Anode: Critical Role of Synthetic Approach.Small science · 2026