Nanoscale

Interfacial stabilization of LATP in lithium-metal batteries by in situ-formed poly(1,3-dioxolane) gel interlayers.

Chenxi Cao, Xinxuan Li, Yufei Wu, Xiumin Liu, Xiaofei Xing, Yingbin Zhuang, Chenchen Mao, Zhe Chen,

MOE Key Laboratory of Resources and Environmental System Optimization, College of Environmental Science and Engineering, North China Electric Power University, Beijing, 102206, P. R. China. shiyongzheng@ncepu.edu.cn. · Institute of Metals and Chemistry, China Academy of Railway Sciences Group Co., Ltd, Beijing, 100081, P. R. China.

Key points

From the paper's conclusion
  • A pDOL/LATP configuration was constructed by the in situ polymerization of a DOL-based precursor containing multiple lithium salts on dense LATP.
  • Li|pDOL/LATP|LFP full cells delivered 166.2 mAh g-1 at 0.2 C and retained 142.2 mAh g-1 after 200 cycles at 0.5 C, corresponding to a 90.4% capacity retention.
  • The pDOL/LATP configuration exhibited limited impedance evolution over 96 h of storage and sustained 1200 h of cycling at 0.1 mA cm-2 and 0.1 mAh cm-2 with low polarization.

Abstract

Poor interfacial contact and reduction-related degradation hinder direct coupling of LATP with Li metal. Herein, a pDOL/LATP configuration was constructed by the in situ polymerization of a DOL-based precursor containing multiple lithium salts on dense LATP. The pDOL interlayer exhibited a room-temperature ionic conductivity of 2.71 mS cm-1, while pDOL/LATP showed an apparent Li+ transference number of 0.92 and an apparent oxidation onset of 4.26 V versus Li/Li+. Li|pDOL/LATP|Li cells exhibited limited impedance evolution over 96 h of storage and sustained 1200 h of cycling at 0.1 mA cm-2 and 0.1 mAh cm-2 with low polarization. Post-cycling Ti 2p XPS spectra showed no detectable Ti3+-related contribution for the LATP surface recovered from the pDOL/LATP cell, whereas a distinct Ti3+-related contribution was observed for the surface recovered from the bare LATP cell. A Li|pDOL/LATP|LFP full cell delivered 166.2 mAh g-1 at 0.2 C and retained 142.2 mAh g-1 after 200 cycles at 0.5 C, corresponding to a 90.4% capacity retention.

Read the paper

Discussion · 1

Science Skim's AI key points, plus readers' public thoughts

Science SkimAI key points
Pinned
  • A pDOL/LATP configuration was constructed by the in situ polymerization of a DOL-based precursor containing multiple lithium salts on dense LATP.
  • Li|pDOL/LATP|LFP full cells delivered 166.2 mAh g-1 at 0.2 C and retained 142.2 mAh g-1 after 200 cycles at 0.5 C, corresponding to a 90.4% capacity retention.
  • The pDOL/LATP configuration exhibited limited impedance evolution over 96 h of storage and sustained 1200 h of cycling at 0.1 mA cm-2 and 0.1 mAh cm-2 with low polarization.