Nanochaperone-mediated dynamic protection of protein conformation enables sustained enzymatic degradation of highly crystalline polylactic acid.
Hongyun Liu, Feihe Ma, Wenyi Gui, Shijia Chen, Linqi Shi
Key Laboratory of Functional Polymer Materials of Ministry of Education, Institute of Polymer Chemistry, State Key Laboratory of Medicinal Chemical Biology, Frontiers Science Center for New Organic Matter, Haihe Laboratory of Sustainable Chemical Transformations, College of Chemistry, Nankai University, Tianjin 300071, P. R. China. feihema@nankai.edu.cn.
Key points
From the paper's conclusion- Here, we report a nanochaperone-based strategy that sustains the activity of the polyester-degrading esterase RPA1511 under high-temperature degradation conditions by dynamically protecting and restoring enzyme conformation.
Abstract
Enzyme-mediated plastic degradation offers a sustainable route for polyester recycling, but its practical efficiency is often constrained by the mismatch between polymer and enzyme dynamics. Efficient enzymatic attack typically requires temperatures near or above the glass transition temperature (Tg), where enhanced polymer-chain mobility improves substrate accessibility, yet such conditions also promote enzyme unfolding, aggregation, and irreversible inactivation. Here, we report a nanochaperone-based strategy that sustains the activity of the polyester-degrading esterase RPA1511 under high-temperature degradation conditions by dynamically protecting and restoring enzyme conformation. The nanochaperone forms thermoresponsive hydrophobic microdomains that recognize thermally perturbed enzyme conformations, suppress irreversible aggregation, and reversibly guide damaged enzymes back toward native, catalytically competent structures. This chaperone-like regulation enhances RPA1511 thermostability, prolongs its thermal activity lifetime, and preserves active-site integrity, enabling approximately 80% degradation of amorphous PDLLA above Tg. By combining alkaline pretreatment with a cyclic "work-rest" heating protocol, highly crystalline PLLA and post-consumer PLA were degraded at 70 °C, achieving >85% degradation within five days with high-purity lactic acid recovery. This work establishes dynamic conformational protection as a new design principle for high-temperature biocatalysis and enzymatic polyester upcycling.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Enzymatic degradation of biopolymers in amorphous and molten states: mechanisms and applicationsFEBS Open Bio · 2025
- Encapsulation of Enzymes in Metal–Organic Frameworks with Dual Thermal Protection for Melt Processing of Self-Biodegradable PlasticsMacromolecules · 2025
- Process-Compatible Immobilization of Thermolabile Enzymes for Self-Degradable Polyesters via Industrial Melt Compounding Conditions.Polymers · 2026
- Structure-Based Discovery and Machine Learning-Aided Design of a Serine Protease for Biocatalytic Recycling of Polylactic AcidACS Sustainable Chemistry & Engineering · 2026
- The Key to Enzymatic Degradation of Polybutylene Terephthalate (PBT): Influence of Semicrystalline Properties on DegradationChemSusChem · 2025
- Dynamic Reorganization of the Entrance Loop Enables Efficient Polylactic Acid Degradation by an Atypical Lid-Free LipaseFermentation · 2026