Leaching behaviour of stereolithography 3D-printed microfluidics.
Volkan Cirik, Lívia Kanizsová, Olga Kočková, N Scott Lynn
FZU - Institute of Physics of the Czech Academy of Sciences, Na Slovance 1999/2, 18200 Prague 8, Czech Republic. lynn@fzu.cz. · Department of Analytical Chemistry, Institute of Macromolecular Chemistry of the Czech Academy of Sciences, Heyrovského nám. 2, Prague 6, 16200, Czech Republic. kockova@imc.cas.cz.
Key points
From the paper's conclusion- These findings highlight the importance of thorough post-processing, careful solvent selection, and optimal fluid flow conditions to improve the chemical stability and biocompatibility of SLA-printed devices in fluidic applications.
Abstract
Stereolithography (SLA) 3D printing has become a standard tool to produce microfluidic structures, thanks to advancements in both 3D printer technology and resin materials. Used across many applications, SLA-printed microfluidics are often exposed to a variety of solvents, giving rise to potential leaching from the printed structure (in the form of unreacted resin components) that can potentially interfere with device functionality. In this study, we investigated the leaching behavior of SLA-printed structures from both external surfaces (under static conditions) and microfluidic surfaces (under flowing conditions). We focused on how leaching is affected by factors such as resin and solvent type, post-processing, fluidic architecture, and internal flow rates. Using a combination of gas chromatography-mass spectrometry (GC-MS) and high-performance liquid chromatography (HPLC) analysis, we identified 15 chemical species consistently found in leachate samples from 4 commercial resins, in the form of monomers and photoinitiators. We found that increased post-processing led to an overall reduction in leaching, with monomers being more affected than photoinitiators. In no case was leaching eliminated. For leaching from microfluidic channels, we found that light treatment did not result in any reduction in leachate levels, which can be attributed to the absorption of light in the external regions of the structure. These findings highlight the importance of thorough post-processing, careful solvent selection, and optimal fluid flow conditions to improve the chemical stability and biocompatibility of SLA-printed devices in fluidic applications.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Defining Operational Limits of Low-Cost MSLA 3D Printing for Microfluidic Systems: Resin Performance, Cell Compatibility, and Fluid Dynamics.ACS omega · 2026
- Biomedical Microfluidic Device Fabrication Using Digital Light Processing and Masked Stereolithography.ACS biomaterials science & engineering · 2026
- Comprehensive Characterisation of Photocurable PEGDA/Gelatine Hydrogels for Extrusion-Based 3D PrintingGels · 2026
- Direct Ink Writing (DIW)-based 3D printing of microscale porous structures using an acrylic resin–fumed silica compositeJournal of Materials Science Composites · 2026
- 3D Printed Microfluidic Device for Combined Thermal and Fluorescence Analysis.Microfluidics and nanofluidics · 2025
- Effect of Post-Curing on the Thermal Behavior and Mechanical Properties of mSLA-Printed Elastic Photopolymer ResinTechnologies · 2026