From the paper's conclusion- This paper examines how different storage conditions affect composite electrodes made from LiNi0.5Mn0.3Co0.2O2 (NMC532) paired with Li6PS5Cl solid electrolyte.
Abstract
Solid-state batteries show promise as future energy storage systems. However, reactions between oxide and thiophosphate materials at their interface often cause decomposition, which shortens cycle life. Until now, these interfaces have mainly been studied electrochemically after cell cycling. Nonetheless, ageing may occur while cycling, or even when composite electrodes, blends of electroactive materials and solid electrolytes, are ground together and stored in a glovebox for a week. This paper examines how different storage conditions affect composite electrodes made from LiNi0.5Mn0.3Co0.2O2 (NMC532) paired with Li6PS5Cl solid electrolyte. Variables like powder versus pellet form, and storage temperatures at 25 °C or 60 °C, were evaluated. After just one week, results showed that storing the material as pellets accelerated decomposition due to the close contact between the active material and the electrolyte. Ageing for only one week significantly reduced the specific charge and increased the polarisation during cycling compared to fresh samples. These changes stem from bulk modifications, including the formation of side phases, like transition metal sulfides and LiCl, and surface reactions producing Li2S. Detailed electrochemical impedance studies revealed that ionic conduction dropped sharply while electronic conductivity rose because of transition metal sulfide formation. The findings highlight how managing electrode ageing is crucial when developing solid-state batteries featuring composite electrodes.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- State‐of‐Charge Dependent Aging Mechanism of Halide‐Based Composite Cathodes for All‐Solid‐State BatteriesAdvanced Energy Materials · 2026
- Revealing interfacial failure mechanism of silicon based all solid state batteries via cryogenic electron microscopyNature Communications · 2025
- Visualizing a Li-Depleted Amorphous Cathode-Electrolyte Interphase in Sulfide Solid-State Batteries Using In Situ Cryogenic Electron Microscopy.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026
- Operando Pressure Monitoring, EIS, and X‐Ray Imaging of Solid‐State Sodium‐Sulfur Batteries — Insights into Chemo‐Mechanical Degradation MechanismsAdvanced Energy Materials · 2026
- Interfacial Resistance and Degradation Behavior of Uncoated Single-Crystal-like and Polycrystalline NCM523 in All-Solid-State Batteries Analyzed by Three-Electrode CellsACS Applied Energy Materials · 2026
- Insight into the Interfacial Evolutions between Halide and Sulfide Solid ElectrolytesACS Energy Letters · 2025