Systemic regulation of depth of discharge mitigates electrochemical-mechanical degradation in 198 Ah Ni-rich lithium-ion batteries.
Chao Wang, Xiaokang Ju, Yongxin Wang, Tianyu Zhu, Hongling Shi, Qian Wang, Zhenjin Liang, Rui Liang,
Sunwoda Mobility Energy Technology Co., Ltd., Shenzhen, 518107, China. hexuan@sunwoda-evb.com. · School of Advanced Energy, Sun Yat-Sen University Shenzhen Campus, Shenzhen, 518107, China. zhoud37@mail.sysu.edu.cn.
Key points
From the paper's conclusion- We demonstrate that restricting the depth of discharge to 94% in 198 Ah industrial NCM batteries effectively mitigates severe anisotropic lattice strain.
Abstract
Rapid electrochemical-mechanical degradation bottlenecks nickel-rich layered cathodes. We demonstrate that restricting the depth of discharge to 94% in 198 Ah industrial NCM batteries effectively mitigates severe anisotropic lattice strain. This systemic intervention strongly suppresses impedance escalation and macroscopic swelling, markedly extending cycle life under rigorous fast-charging and practical mixed-charging protocols.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- The interplay between stack pressure, mechanical expansion and degradation pathways in lithium-ion batteriesNature Energy · 2026
- Exploring Degradation Mechanisms and Recent Developments in High-Nickel Layered Cathodes for Lithium BatteriesElectrochemical Energy Reviews · 2025
- Fast-Discharge-Induced Non-Equilibrium Phase Transition in Ni-Rich Layered Oxide Cathode at High Voltage.Angewandte Chemie (International ed. in English) · 2026
- Multi-Scale Structural Degradation Mechanisms in Ni-Rich NCM Cathodes.Small methods · 2026
- Insights into Degradation Mechanisms and Optimization Strategies for High‐Voltage High‐Ni Cathode MaterialsENERGY & ENVIRONMENTAL MATERIALS · 2026
- Engineering Li+ Transport in Ni-Rich Layered Cathodes Toward Homogenization.Advanced materials (Deerfield Beach, Fla.) · 2026