A bulk-interface synergistic strategy through Ca doping in bulk and Pr-based surface modification for NaNi1/3Fe1/3Mn1/3O2 was developed to overcome its sluggish kinetics. The as-designed cathode delivers excellent performance with a capacity retention of 80.4% after 500 cycles.