Evaluating the effectiveness of coal bottom ash on the mechanical durability and microstructural characteristics of lightweight cellular concrete

Khaled A. Alawi Al-Sodani

Key points

From the paper's conclusion
  • Overall, under the investigated conditions, 5% SF with 10% CBA combination provided balanced mechanical, durability, microstructural, and environmental performance.

Abstract

Coal bottom ash (CBA), a byproduct of coal-based power plants, offers a potential route for reducing the environmental footprint of cement-based materials used to produce lightweight cellular concrete. This study experimentally investigates the influence of CBA as a partial cement replacement on the fresh, mechanical, durability, non-destructive, and microstructural properties of lightweight cellular concrete. For this purpose, six mixtures were developed at a target density of 1600 kg/m 3 . The whole experimental procedure includes a control mix, a mix having 5% silica fume (SF) only (S5CB0) and other mixes containing a constant 5% SF with 0–20% CBA replacement. Compressive strength (CS) and splitting tensile strength tests were performed along with ultrasonic pulse velocity (UPV) to assess the destructive and non-destructive properties. Furthermore, water absorption and rapid chloride permeability were measured to assess durability performance. In addition, scanning electron microscopy and energy-dispersive spectroscopy were evaluated for evaluating microstructural morphology. Based on the results, 10% CBA replacement achieved 8.85% and 10.59% increases in CS over the S5CB0 mix at 28 and 56 days, respectively. The same mix recorded UPV improvements of 11.74% and 8.52%, respectively. Furthermore, the chloride-ion charge passed decreased by 11.55% and 10.87% at 28 and 56 days, respectively, for 10% CBA replacement over the mix having 5% SF only. Microstructural observations and EDS results further supported the formation of a comparatively compact aluminosilicate-rich matrix at moderate CBA content. In addition, the 10% CBA and 5% SF combination reduced embodied CO 2 emissions by almost 8.95% relative to the S5CB0 mix. Overall, under the investigated conditions, 5% SF with 10% CBA combination provided balanced mechanical, durability, microstructural, and environmental performance.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers