Quantitative strengthening and corrosion correlation for partial and full substitution of nickel by nitrogen on AISI 316 stainless steel via VIM
Mostafa M. Shehata, Saeed N. Ghali, Azza Ahmed, Gamila S. Al-Ganainy, Magdy A. M. Ibrahim
Key points
From the paper's conclusion- This study systematically evaluates partial (0.24 N, 6.56 wt% Ni retained) and near-complete (0.52 N, 0.01 wt% Ni) nitrogen substitution in AISI 316 stainless steel, produced via vacuum induction furnace (VIM) under controlled-nitrogen-pressure melting at 18 and 32 bar, respectively.
Abstract
Nickel stabilization of the austenitic phase in stainless steels faces economic and supply-chain pressures, motivating partial or near-complete nickel substitution through nitrogen alloying as an alternative alloy-design strategy. This study systematically evaluates partial (0.24 N, 6.56 wt% Ni retained) and near-complete (0.52 N, 0.01 wt% Ni) nitrogen substitution in AISI 316 stainless steel, produced via vacuum induction furnace (VIM) under controlled-nitrogen-pressure melting at 18 and 32 bar, respectively. Nitrogen addition refined austenite grain size by 53.4% (from 29 to 13.5 μm) and increased dislocation density from 0.13 × 10 14 to 1.97 × 10 14 m −2 , with the 0.52N alloy developing a duplex (γ + α) microstructure. A phase-resolved strengthening model decomposed yield strength contributions into grain refinement, solid-solution, and dislocation mechanisms, achieving good agreement with experimental results. Nitrogen shifted corrosion potential positively, reduced corrosion current density from 9.1 to 2.4 µA cm −2 , and EIS analysis showed the passive film’s charge-transfer resistance rising from 121.5 to 193.5 kΩ cm 2 with a corresponding fall in effective capacitance, while the electrical-equivalent film thickness recalculated from these parameters increases only modestly, from 0.10 to 0.12 nm. Dilatometry revealed a thermal instability window (780–840 °C) unique to the 0.52N alloy, consistent with thermally activated phase evolution within its γ + α duplex microstructure. The 0.24N alloy provides the most balanced combination of strength, ductility, corrosion resistance, and thermal stability among the investigated conditions, while the 0.52N alloy provides the highest strength but also exhibits greater phase complexity and a thermal-instability window; therefore, both alloys require application-specific validation of processing, weldability/forming behaviour, and long-term service performance before industrial deployment.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of nitrogen on grain refinement strengthening in austenitic stainless steel at 77 KScripta Materialia · 2025
- High-Performance Porous High-Nitrogen Nickel-Free Austenitic Stainless Steel via High-Vacuum Reduction Sintering Combined with Solution NitridingMetals · 2026
- Nitrogen and Recrystallization Effects in 316LN Steel: Microstructure Evolution and Cryogenic Deformationsteel research international · 2026
- Research Progress on Hot Deformation Behavior of High Nitrogen Austenitic Stainless Steels: Influence Factors and Microstructure Control of Hot Deformation at High TemperatureMetals · 2026
- Impact of nitrogen fraction in N2-H2 plasma nitrocarburizing on mechanical, tribological, and corrosion performance of AISI 316LSurface and Coatings Technology · 2026
- Short-Term Solution Treatment of LPBF Fe–Cr–Mn–Mo–N High-Nitrogen Duplex Stainless Steel: Microstructure and Tensile Response of Two Initial StatesMetals · 2026