F.-Y. Li, Gui-Yun Song, Qiang Zhang, Mi-Hong Hou
This study explores how EPS with varying molecular weights (MW) adsorb onto polystyrene nanoplastics coated with bare (PS-Bare), carboxylic (PS-COOH), or amine (PS-NH₂) functional groups. Experiments were performed in NaCl and CaCl2 to characterize the formed eco-corona and their impacts on nanoplastics aggregation kinetics. The results show that while eco-corona shares similar chemical compositions, their thickness (ECT) correlates positively with both adsorbed EPS mass and MW. In NaCl, PS-Bare exhibited the narrowest ECT range (0.88–7.17 nm), followed by PS-COOH (1.78–9.43 nm), whereas PS-NH₂ displayed the broadest span (2.33–13.95 nm). The ECT further increased in CaCl2. Enhanced ECT caused higher critical coagulation concentration (CCC). In NaCl, PS-Bare’s CCC rose from 343 mM to 466–1291 mM, and PS-COOH’s from 339 mM to 577–1373 mM. Under 5 mg C L⁻¹ EPS, PS-NH₂ maintained a stable hydrodynamic diameter (Dh ≈ 150 nm) in both NaCl and CaCl2, indicating strengthened steric stabilization. In CaCl2 with 5 mg C L⁻¹ EPS, similar stabilization trends were observed. However, at 10 mg C L⁻¹, high-MW EPS reduced CCC via bridging effects. For PS-NH2, low-MW EPS (5 mg C L⁻¹) increased Dh to 900–1200 nm through charge neutralization and weak steric hindrance. The EPS <3kDa further enlarged Dh to 1400 nm by patch-charge attraction. This study reveals that EPS molecular weight, by regulating eco-corona thickness and surface charge distribution, is a key factor influencing the colloidal stability of nanoplastics.