Enhancement of tribological behavior and microhardness of AISI H13 tool steel by electrochemical boriding
Abdel‐Hamid I. Mourad, Amir A. Mahdy, E.S. Mosa, A. Kandil, M. A. Elhelaly
Al-Azhar University · Tabbin Institute for Metallurgical Studies
Key points
From the paper's conclusion- The findings demonstrated that the phase composition and thickness of the boride coatings are strongly influenced by the immersion time and processing temperature.
Abstract
Abstract Iron boride coatings were developed on AISI H13 hot work tool steel using the electrochemical boriding method at temperatures of 850, 950, and 1050 °C for durations of 2, 4, and 6 h. The process was conducted at a current density of 200 mA/cm 2 , utilizing a powder mixture containing 22.5 wt.% ferroboron (Fe-B), 70 wt.% borax (Na 2 B 4 O 7 ), and 7.5 wt.% ammonium chloride (NH 4 Cl). The obtained coatings were examined using light microscopy (LM), scanning electron microscopy with energy-dispersive spectroscopy (SEM/EDS), and X-ray diffraction (XRD). Metallographic analysis revealed a distinct saw-tooth shaped interface between the boride layer and the underlying transition zone, which was consistent and uniform across the examined area. XRD results revealed the formation of a dual-phase boride layer (FeB/Fe 2 B) with traces of chromium and vanadium borides. The kinetics of the boriding process were evaluated using the classical parabolic growth law, demonstrating a parabolic relationship between boride layer thickness and treatment time. The activation energy required for boron diffusion throughout the boride layer was determined to be 168.4 kJ/mol. Additionally, the microhardness and wear rate were evaluated. The boride layer reached a thickness up to 252 µm and exhibited a microhardness of 1956 ± 67 HV 0.05 , representing an increase of over 300% compared to the quenched and tempered specimens, which had a microhardness of 543 ± 8 HV 0.05 . The findings demonstrated that the phase composition and thickness of the boride coatings are strongly influenced by the immersion time and processing temperature.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Morphological Characterization of Fe2B Borided Layers on AISI 9254 Steel Using Reused Boron Paste: A Classical and Fractal ApproachCoatings · 2025
- Microstructural Changes in Crankshaft Steel After Exposure to BoridingMetals · 2026
- Prediction of Layer Thickness and Stability of Borided Cr–V Steel for Highly Stressed Tubular ComponentsMetals · 2026
- Boride layers on high-carbon high-chromium tool steels: Microstructure-mechanical properties relationshipJournal of Materials Research and Technology · 2025
- Effect of Pack Boriding on the Surface, Wear, Corrosion, and Mechanical Properties of AISI 4140 Steelsteel research international · 2026
- Impact of duplex plasma nitriding and AlCrN coating on mechanical, tribological, and corrosion properties of H13 tool steelJournal of Materials Research and Technology · 2025