From the paper's conclusion- These results collectively highlight the critical role of scaffold composition and processing parameters in engineering 3D neural tissue scaffolds, with the optimized 70:30-10 min scaffold emerging as a promising candidate for advanced neural tissue engineering applications.
Abstract
A three-dimensional (3D) scaffold that enables optimal cell-matrix interactions is essential for developing physiologically relevant neural tissue models. In this study, wet electrospinning was optimized to fabricate nanofibrous PCL/gelatin scaffolds with a well-controlled 3D architecture, using centrifugal force to tune scaffold morphology, porosity, and mechanical properties. The effects of centrifugal force intensity (5000 vs. 10,000 rpm) and application time (5 vs. 10 min) were systematically investigated. Scaffolds fabricated at 5000 rpm exhibited poor structural integrity and were excluded from further analysis. Among scaffolds produced at 10,000 rpm, blends of PCL/gelatin at 70:30 and 60:40 demonstrated excellent porosity (98.1 ± 1.9% and 97.3 ± 1.1%, respectively) and favorable fiber architecture. The 70:30-10 min scaffold achieved the highest tensile strength (57.03 ± 1.50 kPa) and modulus (53.00 ± 2.00 kPa), aligning with the physiological range of neural tissues. MTT assays confirmed robust biocompatibility, with C6 glial cell viability increasing by + 4.30% on the 70:30-10 min scaffold and + 5.88% on the 60:40-10 min scaffold over 14 days. Although the 70:30-5 min scaffold showed the highest proliferation (+ 12.16%), the 10-min variant was selected for detailed morphological evaluation due to its superior mechanical performance and structural uniformity. DAPI and H&E staining further validated the enhanced cell aggregation, ECM deposition, and neural-like morphology within the 70:30-10 min scaffold. These results collectively highlight the critical role of scaffold composition and processing parameters in engineering 3D neural tissue scaffolds, with the optimized 70:30-10 min scaffold emerging as a promising candidate for advanced neural tissue engineering applications.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Core-shell electrospinning combined with sacrificial templating for fabrication of dual-functional porous fibrous scaffoldsInternational Polymer Processing · 2026
- Three‐Dimensional Electrospun Nanofiber Scaffolds: Fabrication Methods and Biomedical ApplicationsMacromolecular Bioscience · 2026
- Nonwoven nanofibrous PLA/SiO₂ -gelatin/hydroxyapatite hybrid scaffolds by two-nozzle electrospinning: bone tissue engineering applicationsBiomedical Materials · 2026
- Shear-Thinning Composite Hydrogel Incorporating Polycaprolactone (PCL) Short Nanofibers for Cell Therapy Applications.Journal of biomedical materials research. Part B, Applied biomaterials · 2026
- Multifunctional pDA@MXene-enriched silk fibroin/PLLA nanofibrous scaffold with local piezoresponse for neural tissue engineering.Journal of biomaterials science. Polymer edition · 2026
- Fabrication of 3D monolayer nanofiber structures via capillary induced bending and fusion.Biofabrication · 2026