Adhesive bond durability and corrosion resistance of AA6060-T6 flash-PEO treated in Mo-Si solutions.
Dominic Shore, Junia C Avelar-Batista Wilson, Nicolas Laugel, Allan Matthews, Aleksey Yerokhin
Department of Materials, University of Manchester, Manchester, UK. · BCW Treatments Ltd, Burnley, UK.
Key points
From the paper's conclusion- All studied flash-PEO coatings performed well in lap shear tests, exhibiting adhesive strength comparable to that of sealed SAA films and demonstrated equivalent or enhanced bond durability when tested after 1008-h Sea Water Acetic Acid Test exposure, indicating satisfactory resistance to moisture and corrosion with preferential adhesive fracture.
Abstract
Aluminium adhesive bonding is a key enabler in lightweighting engineering structures, directly influencing global energy consumption and carbon emissions. Plasma electrolytic oxidation (PEO) has recently emerged as an environmentally friendly alternative to industry-standard sulphuric acid anodising (SAA) surface preparation prior to bonding. However, little is known about the longer-term durability of adhesively bonded PEO-treated structures. Here, AA6060-T6 Al alloy samples were subjected to unconventionally brief 70-s flash-PEO treatments using high-frequency 2.5 kHz unipolar and bipolar pulsed polarisation in aqueous alkaline electrolytes containing Na2SiO3 and optionally Na2MoO4. Molybdate addition and bipolar polarisation improved uniformity and corrosion resistance of thin, ~1 μm, oxide layers produced. All studied flash-PEO coatings performed well in lap shear tests, exhibiting adhesive strength comparable to that of sealed SAA films and demonstrated equivalent or enhanced bond durability when tested after 1008-h Sea Water Acetic Acid Test exposure, indicating satisfactory resistance to moisture and corrosion with preferential adhesive fracture. Comparable to SAA, the long-term bonding performance of flash-PEO treatments highlights their potential as a sustainable surface preparation route for aluminium adhesive bonding.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of Silane Sol Sealing Treatment on the Anti-Corrosion of Micro-Arc Oxidation CoatingMolecules · 2026
- Hydrogen embrittlement susceptibility of AA7075 aluminum alloy subjected to continuous retrogression and re-aging treatment in an aggressive acidic chloride environmentDiscover Materials · 2026
- Quantitative Design and Residual Strength Assessment of Adhesive-Rivet Hybrid Repairs for Perforated Aluminum Alloy Plates.Polymers · 2026
- Influence of Zirconium Addition on Heat Treatment Response, Microstructure, and Corrosion Resistance of AA7075 Alloy for Aerospace Applications.Materials (Basel, Switzerland) · 2026
- Creating Stronger GCFRP /Alloy Steel Joints for Manufacturing High‐Performance Sucker Rod Through Effective NaOH Anodizing and Simple Resin Pre‐Coating MethodsPolymer Composites · 2026
- Joining of Al 5052 Alloy to Advanced High-Strength Steel Sheets of Dissimilar Thickness Using Laser-Assisted Friction Stir Welding.Materials (Basel, Switzerland) · 2026