Efficient dissociation of ultra-high-strength bamboo original fibers via deep eutectic solvent pretreatment for sustainable composite reinforcement.
Ziliang Dai, Lili Zhang, Juan Yu, Enqing Zhu, Rui Wang, Jiao Meng, Muhammad Wajid Ullah, Khalid Ali Khan,
Jiangsu Co-Innovation Center of Efficient Processing and Utilization of Forest Resources, International Innovation Center for Forest Chemicals and Materials, College of Light Industry and Food Engineering, College of Chemical Engineering, College of Materials Science and Engineering, Nanjing Forestry University, Nanjing, China. · Center of Bee Research and its Products (CBRP), Biology Department, College of Science, King Khalid University, P.O. Box 9004, Abha, Saudi Arabia.
Key points
From the paper's conclusion- Here, we develop a mild "top-down" strategy to efficiently dissociate intact bamboo original fibers (BpOFs) from pretreated natural bamboo using a deep eutectic solvent (ChCl/OA-DES) treatment at 110 °C for 1 h.
Abstract
Sustainable structural fibers are highly desirable because many conventional high-performance fibers are neither renewable nor biodegradable. Bamboo original fibers, which possess a natural hollow vascular bundle architecture, represent a promising biomass-derived reinforcement but are difficult to isolate without damaging their structure. Here, we develop a mild "top-down" strategy to efficiently dissociate intact bamboo original fibers (BpOFs) from pretreated natural bamboo using a deep eutectic solvent (ChCl/OA-DES) treatment at 110 °C for 1 h. The treatment selectively weakens parenchyma cell cohesion (elastic modulus reduced from 6.24 to 3.14 GPa) while preserving fiber cell stiffness (15.04 to 15.92 GPa), enabling rapid separation of vascular bundles through subsequent CH₃COOH/H₂O₂ delignification and simple roller compaction. Controlled hydrogen-bond reconstruction during drying enhances mechanical performance, yielding fibers with an apparent tensile strength of 1947 ± 217 MPa while retaining the native hollow structure. Analysis of the load-bearing cell wall further reveals an intrinsic cell-wall stress of 2636 ± 197 MPa, indicating highly efficient stress transfer within the cellulose framework. The preserved tubular architecture provides low density, flexibility, and favorable interfacial interactions with polymer matrices. When incorporated into epoxy resin, BpOFs enhance bending strength and impact resistance, demonstrating their potential as lightweight, renewable reinforcement for high-performance composites.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Achieving High Strength and Modulus in Bamboo/Glass Fiber Hybrid Composites Enabled by Synergistic Interfacial Design.Polymers · 2026
- Vacuum Heat Treatment Regulates the Bamboo-Epoxy Interface: Balancing Mechanical Performance and Thermal Stability.Polymers · 2026
- Extraction of bamboo cellulose via sequential hydrated alkaline-acidic deep eutectic solvent pretreatmentDiscover Applied Sciences · 2026
- DES-separated bamboo lignin-reinforced DES gels with high conductivity, strength, flexibility, and environmental stabilityGreen Chemistry · 2026
- Facile Exfoliation of Silk Nanofibrils Enabled by Hydrogen Bond Network Reconfiguration in Deep Eutectic Solvent/Water SystemsBiomacromolecules · 2025
- Effect of Over‐Mercerization on the Interfacial Bonding and Mechanical Integrity of Bamboo Fiber/Epoxy CompositesSPE Polymers · 2026