◆ Nature Communications2025-10-31· Electrode

Lithium diffusion-controlled Li-Al alloy negative electrode for all-solid-state battery

Yuju Jeon, Dong Ju Lee, Hongkui Zheng, Sesha Sai Behara, Jung-Pil Lee, Junlin Wu, Feng Li, Wei Tang, Lanshuang Zhang, Yu‐Ting Chen, Dapeng Xu, Ji Young Kim, Min‐Sang Song, Anton Van der Ven, Kai He, Zheng Chen

原始摘要(英文原文)· Original abstract
Abstract Metal alloy negative electrodes are promising candidates for lithium all-solid-state batteries due to their high specific capacity and low cost. However, chemo-mechanical degradation and atomic transport limitations in the solid state remain unresolved challenges. Herein, we demonstrate a lithium-aluminum alloy negative electrode design (Li x Al 1 , x = molar ratio of lithium to aluminum) based on a comprehensive understanding of the underlying diffusion mechanisms within the lithium-poor α (0 ≤ x ≤ 0.05) and lithium-rich β phases (0.95 ≤ x ≤ 1). The lithium-aluminum alloy negative electrodes with a higher lithium to aluminum ratio facilitate lithium migration through the β-LiAl phases, which serve as highly lithium-conductive channels with a lithium diffusion coefficient that is ten orders of magnitude higher than that of the α phase. In addition, a bulk dense negative electrode and an intimate negative electrode-electrolyte interface is demonstrated in the cross-sections of the lithium-aluminum alloy negative electrodes. Consequently, a high-rate capability of 7 mA cm −2 is attained in LiNi 0.8 Co 0.1 Mn 0.1 O 2 -based full-cell operation. The optimal cell configuration of Li 0.5 Al 1 | |LiNi 0.8 Co 0.1 Mn 0.1 O 2 shows stable lithium reversibility during 2000 cycles with a capacity retention of 83% at 4 mA cm −2 with a LiNi 0.8 Co 0.1 Mn 0.1 O 2 loading of 5 mAh cm −2 .
读原文 · Read the paper ↗

AI 追问PRO

登录后使用 AI 追问

讨论区

登录后参与讨论

相关论文 · Related

Lithium diffusion-controlled Li-Al alloy negative electrode for all-solid-state battery — 科研速览 Science Skim