Membrane-free redox flow battery with polymer electrolytes
Rajeev K. Gautam, Xiao Wang, Jianbing Jiang
University of Cincinnati
Key points
From the paper's conclusion- Here we show that, at 0.5 M 2,4,6-tri-(1-cyclohexyloxy-4-imino-2,2,6,6-tetramethylpiperidine)−1,3,5-triazine, the battery with solid polymer electrolyte exhibits capacity retentions of 90.7% and 81.78% and Coulombic efficiencies of 95.4% and 96.7% under static and flow conditions, respectively.
Abstract
Li metal-based nonaqueous batteries are valued for high voltage and energy density, but face challenges like Li instability, volatile electrolytes, and costly ion-exchange membranes. To address these, we develop a membrane-free battery employing an ion-immobilized polymer electrolyte as anolyte and organic solvent as catholyte. Two polymer electrolytes are created for Li negative electrode: solid polymer electrolyte of polyvinylidene fluoride-co-hexafluoropropylene and gel polymer electrolyte with polypropylene carbonate. While the solid-state electrolyte offers an initial approach, it is associated with slower Li+ ions diffusion and lower ionic conductivity. The gel polymer electrolyte, specifically developed to overcome these limitations, improves Li+ diffusion, mass transport, and energy density. These anolytes are coupled with 2,4,6-tri-(1-cyclohexyloxy-4-imino-2,2,6,6-tetramethylpiperidine)−1,3,5-triazine in organic solvents (fluoroethylene carbonate and tetra (ethylene glycol) dimethyl ether) as catholytes, forming membrane-free batteries with solid polymer electrolyte and gel polymer electrolyte. Here we show that, at 0.5 M 2,4,6-tri-(1-cyclohexyloxy-4-imino-2,2,6,6-tetramethylpiperidine)−1,3,5-triazine, the battery with solid polymer electrolyte exhibits capacity retentions of 90.7% and 81.78% and Coulombic efficiencies of 95.4% and 96.7% under static and flow conditions, respectively. The battery with gel polymer electrolyte exhibits capacity retentions of 96.8% and 78.8% and Coulombic efficiencies of 97.8% and 98.4%. These results highlight the polymer electrolyte strategy’s potential for enhancing battery performance and safety. Nonaqueous redox flow batteries face challenges like costly membranes and unstable electrolytes. Here, authors develop a membrane-free battery using a polypropylene carbonate gel polymer electrolyte with Li anode and Tri-TEMPO catholyte, achieving a high voltage of 3.45 V, capacity retention of 96.8%, and efficiency of 98.4%.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Covalently Integrated MXene-Fluorinated Polymer Electrolytes for 714 Wh Kg-1 Lithium-Metal Batteries.Advanced materials (Deerfield Beach, Fla.) · 2026
- Nonaqueous Redox Flow Batteries: Opportunities and Challenges for Sustainable Energy Storage.Chemical reviews · 2026
- Potential Posolytes for Aqueous Organic Redox Flow BatteriesAdvanced Energy Materials · 2025
- Fluorine-free gel polymer electrolyte for lithium oxide-rich solid electrolyte interphase and stable Li metal batteriesNature Communications · 2025
- Toward sustainable lithium batteries: From high-fluorine to fluorine-free electrolyte designeScience Energy · 2026
- Stable Li Plating/Stripping in LiPF6-Cyclic Ether-Based Electrolytes.Journal of the American Chemical Society · 2026