BDJ open

Biomodifying effect of rutin extracted from Dimorphandra gardneriana on tensile strength and color change of dentin collagen.

Lara R Aragão, Isabely B Freitas, Selene M de Morais, Solange de O Pinheiro, Ícaro G P Vieira, Wildson M B da Silva, Paulo G B Silva, Marcelo V S Lemos,

Master in Dental Sciences, University Christus (UNICHRISTUS), Fortaleza, Brazil. · School of Dentistry, University Christus Christus (UNICHRISTUS), Fortaleza, Brazil.

Key points

From the paper's conclusion
  • Conclusions Within the limitations of this in vitro study, rutin increased the immediate tensile strength of demineralized dentin collagen, whereas no significant differences in color change were observed among the treatments under the conditions evaluated.

Abstract

OBJECTIVE: To evaluate the effect of rutin extracted from Dimorphandra gardneriana on the tensile strength and color changes of demineralized dentin collagen. METHODS: Two independent experiments were conducted using 244 sound human third molars. For quantitative color analysis, 204 teeth were used to prepare 204 dentin discs, which were allocated to 12 groups (n = 17). For tensile strength analysis, 40 teeth were used to prepare 120 rectangular dentin specimens, which were allocated to 12 groups (n = 10). Specimens were completely demineralized in 10% phosphoric acid and treated with distilled water (control) or aqueous rutin solutions (0.004%, 0.008%, or 0.0125%) for 1, 30, or 60 min. Color changes (ΔL*, Δa*, Δb*, and ΔE*ab) were assessed spectrophotometrically before and after biomodification, and tensile strength was measured using a universal testing machine. Data were analyzed using two-way ANOVA followed by the Student-Newman-Keuls test when significant effects were detected (α = 0.05). RESULTS: No significant effects of treatment, biomodification time, or their interaction were observed for ΔL*, Δa*, Δb*, or ΔE*ab (p > 0.05). Rutin-treated specimens showed significantly higher tensile strength than control specimens (p < 0.05), whereas no significant differences were observed among the rutin concentrations (p > 0.05). Neither biomodification time nor the treatment × time interaction significantly affected tensile strength (p > 0.05). CONCLUSIONS: Within the limitations of this in vitro study, rutin increased the immediate tensile strength of demineralized dentin collagen, whereas no significant differences in color change were observed among the treatments under the conditions evaluated.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers