Machine-Learning-Guided Molecular Design for Dynamic Self-Activating Interface toward Ah-Level Anode-Free Zn-I2 Pouch Cells.
Jia Wu, Shan Guo, Yuren Liu, Qianyi Qu, Shuquan Liang, Guozhao Fang
School of Materials Science and Engineering, Key Laboratory of Electronic Packaging and Advanced Functional Materials of Hunan Province, Central South University, Changsha410083, P. R. China. · Guizhou Provincial University Key Laboratory of High Performance Battery Materials, College of Materials and Metallurgy, Guizhou University, Guiyang550025, P. R. China.
Key points
From the paper's conclusion- Here, we integrate machine-learning-guided polyiodide regulation with dynamic interfacial reconstruction to establish a self-activating Zn deposition pathway for reversible anode-free Zn-I2 cells.
Abstract
Anode-free Zn batteries are attractive for zero-excess-Zn operation and maximized anode utilization, but reversible high-areal-capacity Zn plating/stripping over large hostless interfaces remains difficult, especially in Ah-level Zn-I2 pouch cells where polyiodide shuttling accelerates capacity decay and corrodes the nascent anode interface. Here, we integrate machine-learning-guided polyiodide regulation with dynamic interfacial reconstruction to establish a self-activating Zn deposition pathway for reversible anode-free Zn-I2 cells. DFT-supervised screening reveals multidentate weak O-C-H···I interactions and chain-assisted confinement as key molecular design principles for polyiodide confinement, guiding the selection of polyethylene glycol 4000 (PE4000). More importantly, PE4000 gates trace reversible Sn/Sn2+ interfacial conversion, enabling dynamic Zn-Sn reconstruction, persistent zincophilic sites, and orientation-regulated Zn nucleation/growth during repeated plating/stripping. Consequently, the optimized anode-free Zn-I2 cells sustain 16,000 cycles at 10 mA cm-2. Single-layer pouch cells operate for over 3000 cycles at 4.65 mAh cm-2, with recovered Sn remaining reusable for another 1000 cycles. Ah-level pouch cells further deliver 2390 Ah cumulative capacity over 2800 cycles. This work establishes a system-level interface-matching strategy for practical high-utilization anode-free batteries.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Bidirectional Interfacial Chemical Regulation Enables Durable Aqueous Zn‐I 2 BatteriesRare Metals · 2026
- Machine Learning-Driven Alloy Anode Accompanied by Interfacial Kinetic Compensation Design Toward High-Rate Zinc Pouch Cells.Angewandte Chemie (International ed. in English) · 2026
- Dynamically Adaptive Interfacial Chemistry via Molecular Programming for Sustainable Zn BatteriesJournal of the American Chemical Society · 2026
- Separator-free aqueous zinc–iodine batteries: an in situ dual-confinement interface enabling electrostatic reversible polyiodide capture/releaseEnergy & Environmental Science · 2026
- Molecular/Ionic Coupling Enables a Cycling-Evolved Gradient Interphase for Durable Zinc Metal Anodes.The journal of physical chemistry letters · 2026
- Machine learning-guided electrolyte–interface co-design for Li-based anode-free batteries: Toward a predictive framework for stable metal depositionJournal of Power Sources · 2026