Shenzhen All-Solid-State Lithium Battery Electrolyte Engineering Research Center, Key Laboratory of Electrocatalytic Materials and Green Hydrogen Technology of Guangdong Higher Education Institutes, Shenzhen Key Laboratory for Graphene-based Materials Institute of Materials Research, Tsinghua Shenzhen International Graduate School, Tsinghua University, Shenzhen518055, China. · Nanoyang Group, Tianjin Key Laboratory of Advanced Carbon and Electrochemical Energy Storage, State Key Laboratory of Chemical Engineering and Low-Carbon Technology, School of Chemical Engineering and Technology, National Industry-Education Platform for Energy Storage, and Collaborative Innovation Center of Chemical Science and Engineering, Tianjin University, Tianjin300072, China.

Key points

From the paper's conclusion
  • Here, we propose an interphase catalysis strategy for solid–solid sulfur conversion by transforming discrete catalyst/reactant interfaces into a chemically integrated reaction interphase.

Abstract

Weak solid-solid contact with limited chemical and transport continuity is a common bottleneck in solid-state batteries, particularly in all-solid-state lithium-sulfur batteries (ASSLSBs), where Li2S/S8 conversion requires catalytic acceleration but lacks a continuous solid-state catalytic pathway. Here, we propose an interphase catalysis strategy for solid-solid sulfur conversion by transforming discrete catalyst/reactant interfaces into a chemically integrated reaction interphase. WO3 is identified as a suitable oxide to construct such a metastable mixed-anion S-W-O catalytic interphase on Li2S based on the work-function difference between the metal oxide catalyst and Li2S/S8, which serves as a practical screening rationale for evaluating the relative tendency toward sulfur-oxygen coordination exchange. The interphase contains unsaturated W centers and a polarized electronic environment, enabling coupled electron/Li+ transport and dynamically regulating sulfur redox through coupled sulfur-species exchange. This integrated interphase further stabilizes cathode interfaces during repeated Li2S/S8 conversion. As a result, the optimized cathode sustains stable cycling over 15000 cycles at 10 C and a temperature of 60 °C. A record-high Li2S loading of 30 mg cm-2 with an areal capacity of 21.2 mAh cm-2 is also achieved, demonstrating interphase catalysis as an effective route to overcome solid-state sulfur-conversion limitations in practical ASSLSBs.