Lowering the δ-to-α Phase-Transition Barrier via a Transient Vapor Mediator in Perovskite Formation.
Weiwei Chen, Jinshuai Zhang, Zehuan Jia, Zijian Xu, Haotong Zou, Wei Peng, Lianyou Tang, Huitian Guo,
Hefei National Research Center for Physical Sciences at the Microscale, University of Science and Technology of China, Hefei230026, China. · State Key Laboratory of Precision and Intelligent Chemistry, Department of Materials Science and Engineering, University of Science and Technology of China, Hefei230026, China.
Key points
From the paper's conclusion- By incorporating Pb(SCN)2 during the coevaporation of inorganic precursors, the resulting framework exhibits modified porosity that facilitates the infiltration of organic salts and lowers the activation energy for the solid-state δ-to-α phase transition.
Abstract
Hybrid sequential deposition (HSD) remains a practical pathway for the scalable fabrication of perovskite photovoltaics, though it is frequently constrained by the formation of dense evaporated precursor frameworks and the associated kinetic limitations of the subsequent solid interdiffusion. These constraints often manifest as incomplete conversion and vertical inhomogeneity in the resulting perovskite film. Herein, we report a transient vapor-deposited mediator (TVM) strategy that translates the principles of liquid-phase mediator engineering to a vapor-phase process. By incorporating Pb(SCN)2 during the coevaporation of inorganic precursors, the resulting framework exhibits modified porosity that facilitates the infiltration of organic salts and lowers the activation energy for the solid-state δ-to-α phase transition. The elimination of the mediator under ambient humidity is accompanied by the egress of FASCN-related volatile species, promoting more complete and uniform conversion through the full film thickness with reduced residual PbI2 and lower trap density. This TVM process enables solar cells' power-conversion efficiency to increase from 22.3% to 25.2% and yields enhanced operational robustness, retaining 91% of initial performance after 1200 h of thermal aging at 85 °C and 95% after 1600 h of continuous maximum power point tracking under illumination.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Optimal perovskite vapor partitioning on textured silicon for high-stability tandem solar cellsScience · 2025
- Laser-Defined Reaction Topology Enables Controllable Solid-State Transformations for Scalable Perovskite Photovoltaics.Advanced materials (Deerfield Beach, Fla.) · 2026
- Precursor Stabilization Strategies via Vapor–Solid Reaction for Reproducible and High-Efficiency Vapor-Deposited Perovskite Solar CellsACS Nano · 2026
- A Vapor‐Assisted Repair Strategy for Printing Durable and Reproducible Perovskite PhotovoltaicsAdvanced Functional Materials · 2026
- Controllable Growth of Micron-Thick Films for Bifacial Perovskite Solar CellsACS Energy Letters · 2026
- Liquid-derived, solvent-free vapor-mediated dimensional reconstruction yields a record fill factor in inverted perovskite solar cellsNature Communications · 2026